BFe10-1.6-1 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 5, row 11, designation T70620
PDF page references
11
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Fe1.5 ~ 1.8
Mn0.5 ~ 1.0
Pb≤ 0.03 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Zn≤ 0.2 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T 5231-2012, Table 5, row 11, designation T70620; scanned PDF, PDF physical page 11. Cu is balance. Ni+Co is a combined range and must not be split into individual Ni or Co limits. Dashes mean unspecified and are not replaced with zero. Total table-listed impurities ≤0.4%, subject to the applicable table notes. This standard provides the grade-composition basis for wrought copper-nickel alloys; actual supply and cold-heading suitability require separate confirmation.

Combined limits

Combined-element limits
  • Requirement
    Table 5: Ni+Co total
    Element coefficient
    Ni
    1
    Co
    1
    Lower limit
    9.0
    Upper limit
    11.0
Elements requiring measured values from the same heat
  • Ni
  • Co

Verification notes

Manual cell-by-cell check of Table 5 in the scanned standard original; cross-column elements, summed compositions and footnotes were checked.
WhatsApp Technical enquiry →