← BackMaterial grade directory

B8CA

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for B8CA →

B8CA · ASTM A193/A193M-26

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results.

Material category
Stainless steel
Material form
Bolting material for high-temperature or high-pressure service
Standard edition
ASTM A193/A193M-26
Table / clause
Table 1 and applicable footnotes A, B, E, F, G
PDF page references
3、5
Unit
Mass fraction (wt%)
Analysis type
Heat analysis
UNS identifier in the original table
S34700 (designation correspondence within the same source)
Class identifier in the same original table row
1 / 1A / 1D / 2; Parallel identification in the same row; specific grade, Class and properties must be confirmed separately.

Carbon-equivalent reference

The composition inputs and formula applicability for A193 carbon-equivalent calculations have not been specifically verified; no calculation is provided.

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr17.0 ~ 19.0
Ni9.0 ~ 12.0
Nb≤ 1.1 (lower limit subject to coupled conditions)

Composition linkage limits

Applicable conditions and limitations

ASTM A193/A193M-26, Table 1: heat-analysis mass fractions in wt%; single values are maxima unless a range or minimum is stated. Ellipses indicate no requirement and are not entered as zero.

Intentional additions of Bi, Se, Te and Pb are prohibited; this does not mean that measured contents of these elements are zero.

Product-analysis tolerances in Table 1 are applied separately and are not added in advance to the heat-analysis ranges.

Only chemical composition has been checked in this record. Class, heat treatment, dimensions and inch-pound or metric properties require separate confirmation. This is not a guarantee of cold-heading suitability, finished-product properties or actual supply.

Dynamic stabilization minima must be checked jointly using C or C+N and Nb/Ti from the same analysis. Missing values are not replaced by zero, and the conditions are not converted into fixed minima.