← BackMaterial grade directory

B25

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for B25 →

B25 · GB/T 5231-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2001
Table / clause
Table 4 and footnotes
PDF page references
1、3、4、5、6、7、8、9、10、11、12、13、14

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Fe≤ 0.5 (lower limit not stated)
Mn≤ 0.5 (lower limit not stated)
Zn≤ 0.3 (lower limit not stated)
Pb≤ 0.005 (lower limit not stated)
Si≤ 0.15 (lower limit not stated)
P≤ 0.01 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Mg≤ 0.05 (lower limit not stated)
Sn≤ 0.03 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Under 2.2, elements with specified lower and upper limits are alloying constituents; a single value is a minimum for copper and a maximum for other elements. A dash means unspecified; it is not entered as zero; Cu+Ag and Ni+Co are subject to combined ranges and are not converted into independent element ranges. The balance remains a balance; subtracting independent maxima does not establish a guaranteed range. Total impurities include all relevant impurities; The sum of listed elements is only a necessary condition and cannot replace complete impurity analysis. Product forms in the original document define the applicable wrought-product scope; they do not establish confirmed supply of cold-heading wire or final properties. Cu is the balance. Note 1: Bi/As/Sb need not be analyzed; the supplier guarantees that the limit is not exceeded.

Combined limits

Combined-element limits
  • Element coefficient
    Ni
    1
    Co
    1
    Lower limit
    24.0
    Upper limit
    26.0
    Requirement
    Total Ni + Co
Elements requiring measured values from the same heat
  • Co
  • Ni

Verification notes

The official GB/T 5231—2001 tables 1–4 and applicable footnotes were checked row by row against the source. The condition conflict for seven grades whose Fe content is incompatible with non-magnetic requirements is retained; it is not applied automatically.

B25 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 5, row 5, designation T71200
PDF page references
11、12

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Fe≤ 0.5 (lower limit not stated)
Mn≤ 0.5 (lower limit not stated)
Pb≤ 0.005 (lower limit not stated)
P≤ 0.01 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Mg≤ 0.05 (lower limit not stated)
Si≤ 0.15 (lower limit not stated)
Zn≤ 0.3 (lower limit not stated)
Sn≤ 0.03 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T5231—2012, Table 5, row 5, designation T71200. Cu is the balance; Ni+Co is a coupled combined range and must not be applied independently to each element. Total impurities under Clause 2.3 are ≤1.8% and include all relevant impurities; a partial sum of listed elements cannot replace complete analysis. Table 5, note a: As/Bi/Sb need not be analyzed, but the supplier must still guarantee that the limit is not exceeded; Unlisted numerical values are not guessed or filled in. This standard covers wrought copper-nickel composition and does not establish actual supply of cold-heading wire.

Combined limits

Combined-element limits
  • Element coefficient
    Ni
    1
    Co
    1
    Lower limit
    24
    Upper limit
    26
    Requirement
    Total Ni + Co
Elements requiring measured values from the same heat
  • Co
  • Ni

Verification notes

Each cell in row 5 of Table 5 in the scanned original, together with applicable footnotes, was checked manually
WhatsApp Technical enquiry →