- Material category
- Stainless steel
- Subcategory
- Special alloy steel
- Material form
- Reference record
- Composition basis
- Manufacturer-published composition range
- Verification status
- Reference data; original source not verified
- Document title
- Stellite6B official web data; accessed2026-10-13
- Table / clause
- Chemical Composition — Stellite6B row; *maximum
- PDF page references
- Manufacturer
- Kennametal Stellite
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Co | Cobalt base (no numerical value stated) |
| Cr | 28 ~ 32 |
| W | 3.5 ~ 5.5 |
| C | 0.9 ~ 1.4 |
| Ni | ≤ 3 (lower limit not stated) |
| Si | ≤ 2 (lower limit not stated) |
| Fe | ≤ 3 (lower limit not stated) |
| Mn | Listed as another element; no numerical value stated |
| Mo | Listed as another element; no numerical value stated |
Applicability and limitations
The archived webpage explicitly calls Alloy6B Stellite6B. This record has been checked against the manufacturer’s official 6B row; do not apply the adjacent Stellite6 row to it.. Asterisks for Ni/Si/Fe represent maximum values of 3/2/3% respectively.; Co is labeled Base; Mn/Mo are listed as other elements with no numerical values.; Other values in the old reference library have no basis in this table; original values are retained in the repair evidence.. The page references AMS5894 but without a specific version; it cannot be claimed that the original text of the standard has been verified..