A576 1524
2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for A576 1524 →A576 1524 · ASTM A576-2025
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Original record status
- Historical-edition reference
- Standard edition
- ASTM A576-17
- Table / clause
- Table 1 · Notes C–G; Clause 1,5,7
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.19 ~ 0.25 |
| Mn | 1.35 ~ 1.65 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
The chemical composition currently shown is transcribed from the original ASTM A576-2017; The original record cites ASTM A576-2025; that original edition remains unavailable, and differences between editions have not been confirmed. ASTM A576-17 applies to hot-finished bars of quality carbon steel; Table 1 specifies heat analysis; This must not be assumed to guarantee the performance of wire rod or finished cold-heading products.. ; Table 1 Note C: Si shall be according to order agreement when required, commonly ≤0.10, 0.10–0.20, 0.15–0.35, or 0.20–0.40%.; Do not enter a fixed Si value if not agreed upon. ; Table 1 Note D: When Cu is required, Cu≥0.20% may be specified, which is a conditional requirement.. ; Notes E/F/G: Pb, B, and Bi/Ca/Se/Te are all applicable only when specified.; Do not automatically add Pb/B lower limits to all grades. ; Clause 7.1 requires reporting the content of Cu/Cr/Ni/Mo/V/Nb; the reporting requirement is not equivalent to the provision of limits for these elements in Table 1.. ; Clause 5.1 allows other chemical ranges to be agreed upon according to Table 2.; Table 2 does not impose additional mandatory limits on every grade in Table 1..
Verification notes
The current chemistry display uses original ASTM A576-2017 data. The source record is labeled ASTM A576-2025; that edition’s original text remains to be obtained, and edition differences have not been confirmed.A576 1524 · ASTM A576-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ASTM A576-17
- Table / clause
- Table 1 · Notes C–G; Clause 1,5,7
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.19 ~ 0.25 |
| Mn | 1.35 ~ 1.65 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
ASTM A576-17 applies to hot-worked bars of quality carbon steel; Table 1 gives ladle chemistry. It must not be assumed to guarantee wire-rod supply or finished cold-heading properties. Table 1 note C: Si, when needed, is agreed at order; common options are ≤0.10, 0.10–0.20, 0.15–0.35 or 0.20–0.40%. Without agreement, do not assign a fixed Si value. Table 1 note D: Cu ≥0.20% may be specified when required; this is conditional. Notes E/F/G: Pb, B and Bi/Ca/Se/Te apply when specified; do not automatically add Pb or a B minimum to all grades. Clause 7.1 requires reporting Cu/Cr/Ni/Mo/V/Nb contents; a reporting requirement does not mean Table 1 sets limits for these elements. Clause 5.1 allows other chemical ranges to be agreed under Table 2; Table 2 is not a mandatory set of additional limits for every Table 1 grade.