← BackMaterial grade directory

A576 1213

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for A576 1213 →

A576 1213 · ASTM A576-2017

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A576-17
Table / clause
Table 1 · Notes C–G; Clause 1,5,7

Carbon-equivalent reference

IIW / CEV:0.1167–0.2967 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33

Applicability and limitations

ASTM A576-17 applies to hot-finished bars of quality carbon steel; Table 1 specifies heat analysis; This must not be assumed to guarantee the performance of wire rod or finished cold-heading products.. ; Table 1 Note C: Si shall be according to order agreement when required, commonly ≤0.10, 0.10–0.20, 0.15–0.35, or 0.20–0.40%.; Do not enter a fixed Si value if not agreed upon. ; Table 1 Note D: When Cu is required, Cu≥0.20% may be specified, which is a conditional requirement.. ; Notes E/F/G: Pb, B, and Bi/Ca/Se/Te are all applicable only when specified.; Do not automatically add Pb/B lower limits to all grades. ; Clause 7.1 requires reporting the content of Cu/Cr/Ni/Mo/V/Nb; the reporting requirement is not equivalent to the provision of limits for these elements in Table 1.. ; Clause 5.1 allows other chemical ranges to be agreed upon according to Table 2.; Table 2 does not impose additional mandatory limits on every grade in Table 1.. ; Table 1, Note H: These grades are usually not produced to the specified Si limits for machinability reasons; do not infer a Si range..

Verification notes

The original standard text of Table 1 and its footnotes has been checked.
WhatsApp Technical enquiry →