A322 94B17 · ASTM A322-1991(R2001)e1

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A322-1991(R2001)e1
Table / clause
Table 1 · Notes A–G
PDF page references
1、2、3

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 1 default Si .15–.35%; Usual Ti addition; B .0005–.003%
IIW / CEV:0.3710–0.5600Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2203–0.3392Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2555–0.3725 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Table 1 default Si .15–.35%; Usual Ti addition not permitted; B upper limit may reach .005%
IIW / CEV:0.3710–0.5600Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2203–0.3492Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2555–0.3725 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser specifies Si≤.10%; Usual Ti addition; B .0005–.003%
IIW / CEV:0.3710–0.5600Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2153–0.3308Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2555–0.3725 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser specifies Si≤.10%; Usual Ti addition not permitted; B upper limit may reach .005%
IIW / CEV:0.3710–0.5600Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2153–0.3408Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2555–0.3725 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.15 ~ 0.2
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni0.3 ~ 0.6
Cr0.3 ~ 0.5
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)
B0.0005 ~ 0.003

Applicability and limitations

Original header A322–91(Reapproved2001)e1; note e1 records correction of Table 1 in year 2004, month 5. The full edition is retained, not represented as 2013/2024. Cast analysis wt%. Note A gives maximum incidental contents for elements not otherwise specified or required: Cu≤.35/Ni≤.25/Cr≤.20/Mo≤.06; explicitly specified alloy ranges take priority. Note F: the purchaser may specify Si≤.10%, usually for severely cold-formed parts; default Si .15–.35%. Select the two conditions separately; this does not establish cold-heading supply availability. Note B: adding Pb .15–.35% requires L identification; not included in ordinary grades. This standard covers hot-worked alloy steel bars; coiled dimensions and applicability require supplier confirmation. Product deviations and other composition agreements referring to A29 require separate verification. Original-table UNS G94171; grade column 94B17. Note G specifies intended boron content: usually .0005–.003%, up to .005% when the usual Ti addition is not permitted. This is not unrestricted widening; conditions remain separate.

Original condition-branch records

Table 1 default Si .15–.35%; Usual Ti addition; B .0005–.003%

ElementComposition requirement
C0.15 ~ 0.2
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni0.3 ~ 0.6
Cr0.3 ~ 0.5
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)
B0.0005 ~ 0.003

Table 1 default Si .15–.35%; Usual Ti addition not permitted; B upper limit may reach .005%

ElementComposition requirement
C0.15 ~ 0.2
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni0.3 ~ 0.6
Cr0.3 ~ 0.5
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)
B0.0005 ~ 0.005

Purchaser specifies Si≤.10%; Usual Ti addition; B .0005–.003%

ElementComposition requirement
C0.15 ~ 0.2
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Ni0.3 ~ 0.6
Cr0.3 ~ 0.5
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)
B0.0005 ~ 0.003

Purchaser specifies Si≤.10%; Usual Ti addition not permitted; B upper limit may reach .005%

ElementComposition requirement
C0.15 ~ 0.2
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Ni0.3 ~ 0.6
Cr0.3 ~ 0.5
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)
B0.0005 ~ 0.005

A condition branch must be selected

Yes

Verification notes

PDF pages 2–3: all 71 UNS and grade entries, plus notes A–G, visually checked item by item.