← BackMaterial grade directory

A322 4120

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for A322 4120 →

A322 4120 · ASTM A322-2013

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C0.18 ~ 0.23
Cr0.4 ~ 0.6
Mn0.9 ~ 1.2
Mo0.13 ~ 0.2
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

Verification notes

The SAE grade column in original G41200 is blank; the previous attribution of direct correspondence to original historical 4120 is withdrawn; An explicit grade basis is still required

A322 4120 · ASTM A322-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C0.18 ~ 0.23
Cr0.4 ~ 0.6
Mn0.9 ~ 1.2
Mo0.13 ~ 0.2
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

Verification notes

The SAE grade column in original G41200 is blank; the previous attribution of direct correspondence to original historical 4120 is withdrawn; An explicit grade basis is still required
WhatsApp Technical enquiry →