← BackMaterial grade directory

A322 4118

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for A322 4118 →

A322 4118 · ASTM A322-2013

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original text of the historical edition verified
Standard edition
ASTM A322-1991(R2001)e1
Table / clause
Table 1 · Notes A–G
PDF page references
1、2、3

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 1 default Si .15–.35%
IIW / CEV:0.3927–0.5700Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2453–0.3483Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2780–0.3887 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser specifies Si≤.10%
IIW / CEV:0.3927–0.5700Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2403–0.3400Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2780–0.3887 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

Applicability and limitations

Original header A322–91(Reapproved2001)e1; note e1 records correction of Table 1 in year 2004, month 5. The full edition is retained, not represented as 2013/2024. Cast analysis wt%. Note A gives maximum incidental contents for elements not otherwise specified or required: Cu≤.35/Ni≤.25/Cr≤.20/Mo≤.06; explicitly specified alloy ranges take priority. Note F: the purchaser may specify Si≤.10%, usually for severely cold-formed parts; default Si .15–.35%. Select the two conditions separately; this does not establish cold-heading supply availability. Note B: adding Pb .15–.35% requires L identification; not included in ordinary grades. This standard covers hot-worked alloy steel bars; coiled dimensions and applicability require supplier confirmation. Product deviations and other composition agreements referring to A29 require separate verification. Original-table UNS G41180; grade column 4118.

Original condition-branch records

Table 1 default Si .15–.35%

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

Purchaser specifies Si≤.10%

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

The verified historical original 1991(R2001)e1 table composition is used for now; The specified 2013(R2018) edition remains unavailable and is not treated as a confirmed same-edition source.

A322 4118 · ASTM A322-2024

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A322-1991(R2001)e1
Table / clause
Table 1 · Notes A–G
PDF page references
1、2、3

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 1 default Si .15–.35%
IIW / CEV:0.3927–0.5700Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2453–0.3483Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2780–0.3887 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser specifies Si≤.10%
IIW / CEV:0.3927–0.5700Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2403–0.3400Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2780–0.3887 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

Applicability and limitations

The chemical composition currently shown is transcribed from the original ASTM A322-1991(R2001)e1. The previous record cited ASTM A322-2024; that original edition remains unavailable, and differences between editions have not been confirmed. The original file header is A322–91(Reapproved2001)e1; note e1 states that Table 1 was corrected in month 5 of 2004. The full edition designation is retained and is not presented as edition 2013/2024. Heat analysis wt%. Note A gives maximum incidental contents for elements not otherwise specified or required: Cu≤.35/Ni≤.25/Cr≤.20/Mo≤.06; explicitly specified alloy ranges take priority. Under note F, the purchaser may specify Si≤.10%, usually for severely cold-formed parts; the default is Si .15–.35%. These two conditions must be selected separately and do not establish availability for cold heading. Under note B, addition of Pb .15–.35% requires the L designation and is not included in an ordinary grade. This standard concerns hot-worked alloy-steel bars. Coiled dimensions and applicability require supplier confirmation. Product-analysis tolerances and other agreed compositions under A29 require separate verification. The original table lists UNS G41180; the grade column gives 4118.

Original condition-branch records

Table 1 default Si .15–.35%

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

Purchaser specifies Si≤.10%

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

The current chemistry display uses original ASTM A322-1991(R2001)e1 data. The source record is labeled ASTM A322-2024; that edition’s original text remains to be obtained, and edition differences have not been confirmed.

A322 4118 · ASTM A322-1991(R2001)e1

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A322-1991(R2001)e1
Table / clause
Table 1 · Notes A–G
PDF page references
1、2、3

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 1 default Si .15–.35%
IIW / CEV:0.3927–0.5700Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2453–0.3483Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2780–0.3887 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser specifies Si≤.10%
IIW / CEV:0.3927–0.5700Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2403–0.3400Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2780–0.3887 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

Applicability and limitations

Original header A322–91(Reapproved2001)e1; note e1 records correction of Table 1 in year 2004, month 5. The full edition is retained, not represented as 2013/2024. Cast analysis wt%. Note A gives maximum incidental contents for elements not otherwise specified or required: Cu≤.35/Ni≤.25/Cr≤.20/Mo≤.06; explicitly specified alloy ranges take priority. Note F: the purchaser may specify Si≤.10%, usually for severely cold-formed parts; default Si .15–.35%. Select the two conditions separately; this does not establish cold-heading supply availability. Note B: adding Pb .15–.35% requires L identification; not included in ordinary grades. This standard covers hot-worked alloy steel bars; coiled dimensions and applicability require supplier confirmation. Product deviations and other composition agreements referring to A29 require separate verification. Original-table UNS G41180; grade column 4118.

Original condition-branch records

Table 1 default Si .15–.35%

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

Purchaser specifies Si≤.10%

ElementComposition requirement
C0.18 ~ 0.23
Mn0.7 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr0.4 ~ 0.6
Mo0.08 ~ 0.15
Cu≤ 0.35 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

PDF pages 2–3: all 71 UNS and grade entries, plus notes A–G, visually checked item by item.