A194 Grade B8ML4CuN · ASTM A194/A194M-2020

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A194/A194M-2020
Table / clause
Table 1 · Footnotes A–I; Scope 1.1–1.5
PDF page references
2、4、5

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Cr17 ~ 19
Ni15 ~ 16.5
Mo3 ~ 4
N≤ 0.045 (lower limit not stated)
Cu4 ~ 5

Applicability and limitations

ASTM A194/A194M—2020 chemical requirements for nut materials, mass fraction wt%; Cold heading supply or finished product strength cannot be directly inferred from the grade composition. Table 1 Note C: Values without a specified lower limit or range are upper limits; Ellipses indicate no requirement; measurement or reporting is not required, and shall not be filled as zero. Table 1 Note A: Intentional addition of Bi/Se/Te/Pb is not permitted; This exception applies only to types where Se is explicitly specified in 6F, 8F, and 8FA; Se shall not be added to all types. Note E: Finished product analysis where S exceeds the upper limit of 0.060% is technically unsuitable; Finished product analysis deviations shall be verified separately according to the original text; heat limits shall not be relaxed. A suffixes, as well as heat treatment, dimensional, and manufacturing requirements, shall be retained separately; grades shall not be merged based on identical composition. The adoption relationship of ASME SA-194 has not been confirmed for this batch; Original texts of 2016, 2023 and 2026 have not been verified; the displayed composition is based only on 2020. The original table explicitly prints the grade as B8ML4CuN; retain the B prefix and do not alter the printed name arbitrarily..