8MNSI7
3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 8MNSI7 →8MnSi7 · EN 10263
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Drawn wire
- Original record status
- Reference transcription of standard
- Standard edition
- BS EN 10263-2:2017
- Table / clause
- Table 2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | 0.9 ~ 1.1 |
| Mn | 1.6 ~ 1.8 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Al | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
BS EN 10263-2:2017; Heat analysis, mass percent; Values without a stated range are maxima; Notes below the table are retained. No edition is stated on the website; Displayed under this source edition; contract applicability is not established
Verification notes
Standard source: BS EN 10263-2:2017 · Table 2View associated products →8MnSi7 · EN 10263-2-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10263-2-2017
- Table / clause
- Table 2 and notes a–f
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Default composition in Table 2, Al deoxidation condition
Default composition in Table 2, Al deoxidation condition; Al is replaced by elements with equivalent effect; the replacement elements and contents require separate verification
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | 0.9 ~ 1.1 |
| Mn | 1.6 ~ 1.8 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Al | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
Heat-analysis mass fractions wt%; See Table 3 separately for product-analysis tolerances. ; Note b permits aluminum to be replaced by other elements with a similar effect; composition of replacement elements must not be inferred before they are identified. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; Residual elements must not impair properties or suitability; unlisted content does not mean zero. ; This standard covers cold heading and cold extrusion; actual delivery condition, dimensions, surface and mechanical properties require separate verification, and no supply product is created automatically.
Original condition-branch records
Default composition in Table 2, Al deoxidation condition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | 0.9 ~ 1.1 |
| Mn | 1.6 ~ 1.8 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Al | ≤ 0.02 (lower limit not stated) |
Default composition in Table 2, Al deoxidation condition; Al is replaced by elements with equivalent effect; the replacement elements and contents require separate verification
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | 0.9 ~ 1.1 |
| Mn | 1.6 ~ 1.8 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
A condition branch must be selected
YesVerification notes
The original Table 2 and footnotes have been checked; Optional additions and agreed provisions require separate confirmation8MnSi7 · DIN EN 10263-2-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10263-2:2018-02
- Table / clause
- Tabelle 2 and footnote a–f; Tabelle 3 product-analysis tolerances require separate verification
- PDF page references
- 1、9
- Unit
- Mass fraction (wt%)
- Analysis type
- Heat analysis
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Default composition in Table 2, Al deoxidation condition
Default composition in Table 2, Al deoxidation condition; Al is replaced by elements with equivalent effect; the replacement elements and contents require separate verification
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | 0.9 ~ 1.1 |
| Mn | 1.6 ~ 1.8 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Al | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
DIN EN 10263-2:2018-02 is the German-language edition of EN 10263-2:2017; This record was verified against heat analysis and footnotes in Table 2 of the official German edition. ; Heat-analysis mass fractions wt%; See Table 3 separately for product-analysis tolerances. ; Note b permits aluminum to be replaced by other elements with a similar effect; composition of replacement elements must not be inferred before they are identified. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; Residual elements must not impair properties or suitability; unlisted content does not mean zero. ; This standard covers cold heading and cold extrusion; actual delivery condition, dimensions, surface and mechanical properties require separate verification, and no supply product is created automatically.
Original condition-branch records
Default composition in Table 2, Al deoxidation condition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | 0.9 ~ 1.1 |
| Mn | 1.6 ~ 1.8 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Al | ≤ 0.02 (lower limit not stated) |
Default composition in Table 2, Al deoxidation condition; Al is replaced by elements with equivalent effect; the replacement elements and contents require separate verification
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | 0.9 ~ 1.1 |
| Mn | 1.6 ~ 1.8 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |