8740H · SAE J1268-2010

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J1268-2010
Table / clause
Table 2 · Notes 1–6; Clause 3/4
PDF page references
1、2、4、5、6

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Open-hearth or basic-oxygen steel: P≤0.030/S≤0.040
IIW / CEV:0.6200–0.8783Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4467–0.5867Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4863–0.6438 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Basic electric-furnace steel: P and S each ≤0.025%
IIW / CEV:0.6200–0.8783Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4467–0.5867Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4863–0.6438 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.37 ~ 0.44
Mn0.7 ~ 1.05
Si0.15 ~ 0.35
Ni0.35 ~ 0.75
Cr0.35 ~ 0.65
Mo0.2 ~ 0.3
Cu≤ 0.35 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)

Applicability and limitations

SAE J1268 MAY2010 official original Table 2 and notes 1–6, ladle analysis (wt%). Note 1 applies within the stated scope: cross-sectional area ≤0.13 m², width 460 mm and piece mass 4.5 t; product deviations are handled separately under J409 and are not added to default limits. Note 2 residual maxima Cu≤0.35/Ni≤0.25/Cr≤0.20/Mo≤0.06 apply only when the element is not specified; listed alloy ranges take priority. Note 3: open-hearth/oxygen steel P≤0.030/S≤0.040; basic electric-furnace steel P and S each ≤0.025. The original note 5 identifies E4340H/E9310H as electric-furnace steel. Note 6: boron steel B 0.0005–0.003%; do not add boron to ordinary grades without B. Retain the explicit H-grade to UNS mappings from the source; do not merge them with grades without H. Hardenability bands, grain size, cold-heading process and supply require separate verification.

Original condition-branch records

Open-hearth or basic-oxygen steel: P≤0.030/S≤0.040

ElementComposition requirement
C0.37 ~ 0.44
Mn0.7 ~ 1.05
Si0.15 ~ 0.35
Ni0.35 ~ 0.75
Cr0.35 ~ 0.65
Mo0.2 ~ 0.3
Cu≤ 0.35 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)

Basic electric-furnace steel: P and S each ≤0.025%

ElementComposition requirement
C0.37 ~ 0.44
Mn0.7 ~ 1.05
Si0.15 ~ 0.35
Ni0.35 ~ 0.75
Cr0.35 ~ 0.65
Mo0.2 ~ 0.3
Cu≤ 0.35 (lower limit not stated)
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Official original Table 2: all 73 rows and footnotes visually checked.

8740H · CHINA STEEL CORPORATION · Bars and Wire Rods Product Catalogue 2014-C1 / 7.1.19 SAE · Alloy steels · H (continued table)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Bars and wire rod
Original record status
Manufacturer source verified
Document edition
CAT.NO.3-BD-01-2014-C1 (stated on the back cover)
Document title
Bars and Wire Rods Product Catalogue
Table / clause
7.1.19 SAE · Alloy steels · H (continued table)
PDF page references
26
Unit
Mass fraction (%)
Analysis type
The original catalogue does not explicitly identify the analysis type for this table
Manufacturer
CHINA STEEL CORPORATION

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.6200–0.8783Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4467–0.5867Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4863–0.6438 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.37 ~ 0.44
Mn0.7 ~ 1.05
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni0.35 ~ 0.75
Cr0.35 ~ 0.65
Mo0.2 ~ 0.3
Cu≤ 0.35 (lower limit not stated)

Applicability and limitations

China Steel bar and wire-rod catalogue CAT.NO.3-BD-01-2014-C1, PDF page 26

printed page 24, 7.1.19 SAE alloy H steel (continued table). The original catalogue does not explicitly identify the analysis type for this table. Historical manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition: residual Cu/Ni/Cr/Mo maxima are added only for elements unspecified in the main table and do not override principal alloy-composition ranges.

Composition conditions

Verification notes

Merged cells in all 28 catalogue tables were reconstructed geometrically, with no missing cells. Original images, continuation pages and notes are recorded; disputed conditions are withheld.