- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original text of the historical edition verified
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、12、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 1.2 ~ 2.0 |
| Mn | ≤ 0.15 (lower limit not stated) |
| Mg | 2.0 ~ 3.0 |
| Cr | 0.16 ~ 0.3 |
| Zn | 5.1 ~ 6.1 |
| Ti | ≤ 0.1 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass fraction %; unspecified elements are not treated as zero. This standard specifies the chemical composition of wrought aluminium and aluminium alloys; it does not automatically establish cold-heading suitability, actual supply, or finished-product performance. Al is the balance; the original table gives no independent numerical range for Al. Individual and total limits for other impurities apply only to the other elements referred to in clause 4.3, not to the sum of all principal alloying elements; a missing impurity test is not zero.
Combined limits
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.1
- Other impurities require technical review
- Yes
Verification notes
The original GB/T 3190—1996, Table 1 is used as an explicitly historical basis; The 2008/2020 edition cited in the original index has not been verified.7A09 · GB /T 3190-2020
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original text of the historical edition verified
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、12、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 1.2 ~ 2.0 |
| Mn | ≤ 0.15 (lower limit not stated) |
| Mg | 2.0 ~ 3.0 |
| Cr | 0.16 ~ 0.3 |
| Zn | 5.1 ~ 6.1 |
| Ti | ≤ 0.1 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass fraction %; unspecified elements are not treated as zero. This standard specifies the chemical composition of wrought aluminium and aluminium alloys; it does not automatically establish cold-heading suitability, actual supply, or finished-product performance. Al is the balance; the original table gives no independent numerical range for Al. Individual and total limits for other impurities apply only to the other elements referred to in clause 4.3, not to the sum of all principal alloying elements; a missing impurity test is not zero.
Combined limits
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.1
- Other impurities require technical review
- Yes
Verification notes
The original GB/T 3190—1996, Table 1 is used as an explicitly historical basis; The 2008/2020 edition cited in the original index has not been verified.7A09 · GB/T 3190—1996
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、12、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 1.2 ~ 2.0 |
| Mn | ≤ 0.15 (lower limit not stated) |
| Mg | 2.0 ~ 3.0 |
| Cr | 0.16 ~ 0.3 |
| Zn | 5.1 ~ 6.1 |
| Ti | ≤ 0.1 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass fraction %; unspecified elements are not treated as zero. This standard specifies the chemical composition of wrought aluminium and aluminium alloys; it does not automatically establish cold-heading suitability, actual supply, or finished-product performance. Al is the balance; the original table gives no independent numerical range for Al. Individual and total limits for other impurities apply only to the other elements referred to in clause 4.3, not to the sum of all principal alloying elements; a missing impurity test is not zero.
Combined limits
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.1
- Other impurities require technical review
- Yes
7A09 · GB /T 3880.1-2012
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | 0.16 ~ 0.3 |
| Cu | 1.2 ~ 2 |
| Fe | ≤ 0.5 (lower limit not stated) |
| Mg | 2 ~ 3 |
| Mn | ≤ 0.15 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.1 (lower limit not stated) |
| Zn | 5.1 ~ 6.1 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.