72BPG

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 72BPG →

72BPG · Kobe Steel manufacturer specification (section 6-4)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Wire rod for prestressed steel wire
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Publication edition not stated in the document
Document title
Wire rod and bar specification tables
Table / clause
6-4
PDF page references
26
Unit
Mass fraction (wt%)
Manufacturer
Kobe Steel

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.8000–0.9433Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.7340–0.8232Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.7600–0.8588Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.7 ~ 0.75
Si0.12 ~ 0.32
Mn0.6 ~ 0.9
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.15 (lower limit not stated)
Cr≤ 0.1 (lower limit not stated)

Applicability and limitations

Original composition for wire rod for prestressing wire in the Kobe Steel catalogue, section 6-4 (PDF page 26), mass fractions wt%; This is not the original JIS/SAE standard. The manufacturer catalogue does not state a publication year; actual supply and application require separate confirmation; This does not establish a supply commitment from Creation Group.

Composition conditions

Verification notes

The original manufacturer catalogue table was checked cell by cell against the boundaries of the PDF table; Added elements without numerical values are retained as text only.