70MN

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 70MN →

70Mn · GB/T 699-2015

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Quality carbon structural steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 699-2015
Table / clause
Table 1 and notes a and b; clauses 6.1.2 and 6.1.3

Carbon-equivalent reference

IIW / CEV:0.8200–1.0367Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.7207–0.8523Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.7600–0.9025Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.67 ~ 0.75
Si0.17 ~ 0.37
Mn0.9 ~ 1.2
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cr≤ 0.25 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)

Applicability and limitations

Table 1 of GB/T699-2015 gives heat-analysis mass fractions wt%; Product-analysis tolerances are listed separately under GB/T222. ; Table 1, note a: Cu≤0.20% for steel intended for hot pressure working; other tabulated cases are ≤0.25%. ; 6.1.2: N≤0.008% applies to basic oxygen steelmaking; analysis may be omitted if the supplier guarantees compliance; Applicability depends on the steelmaking method. ; 6.1.3: for lead-bath-patented wire, Mn0.30–0.60% for 35–85 and Mn0.70–1.00% for 65Mn/70Mn, Cr≤0.10/Ni≤0.15/Cu≤0.20%; P/S follows the corresponding wire standard and must not exceed Table 1. This is a conditional exception, not a general range. ; Elements not specified in the table must not be intentionally added without purchaser consent.

Verification notes

Table 1 and applicable clauses verified

70Mn · GB/T 1222-2016

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 1222-2016
Table / clause
Table 1 · continued table · Notes a/b; 6.1.1–6.1.3

Carbon-equivalent reference

IIW / CEV:0.8200–1.0400Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.7207–0.8532Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.7600–0.9037Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.67 ~ 0.75
Si0.17 ~ 0.37
Mn0.9 ~ 1.2
Cr≤ 0.25 (lower limit not stated)
Ni≤ 0.35 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)

Applicability and limitations

Heat analysis, mass fractions wt%; Product-analysis tolerances are assessed separately under GB/T222 and are not included in this table. ; Table 1, note b: when required by the purchaser and stated in the contract, residual Cu may be ≤0.20%; Default tabulated limit ≤0.25%. ; 6.1.2: oxygen in 40SiMnVBE is ≤0.0015%; oxygen in other alloy spring steels is ≤0.0025%; This limit is not extended to carbon spring steels. ; Unspecified elements do not mean zero; Spring-steel composition does not establish suitability for every cold-headed component; the specific process requires a separate assessment.

Verification notes

Table 1 and its footnotes, and the oxygen-content requirement in 6.1.2, were checked.

70Mn · GB/T 699-1999

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Material form
Quality carbon structural steel (source classification)
Original record status
Original standard verified
Standard edition
GB/T 699-1999
Table / clause
Main-text Table 1, row 31, Table 2 and Clause 6.1.1
PDF page references
5、6
Unit
Mass fraction (%)
Analysis type
Ladle analysis

Carbon-equivalent reference

IIW / CEV:0.8200–1.0367Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.7207–0.8523Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.7600–0.9025Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.67 ~ 0.75
Si0.17 ~ 0.37
Mn0.9 ~ 1.2
Cr≤ 0.25 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)

Applicability and limitations

Edition 1999, main-text Table 1, row 31, unified numerical designation U21702. This record uses the default quality-steel class; heat analysis, mass fraction %. Table 2: for quality steel, P and S are each ≤0.035%; for higher-quality class A, each is ≤0.030%; for special-quality class E, the requirements are P≤0.025% and S≤0.020%. Do not apply A/E limits to the default class. 6.1.1.2—3: scrap-based steelmaking may permit Cu≤0.30%; steel for hot pressure working requires Cu≤0.20%. This record retains the default Cu≤0.25% in Table 1; specific conditions require separate confirmation. 6.1.1.4: Mn/Cr/Ni/Cu for lead-patented steel wire 35—85 has a separate restriction and does not apply to this default structural-steel record. Mechanical properties in Table 3 and 6.4 depend on specimens, dimensions, heat treatment and order requirements. Existing reference properties are not upgraded to universal guarantees by this composition review.

Verification notes

1999 original Tables 1/2 and clause 6.1.1 checked line by line.
WhatsApp Technical enquiry →