65MN
11 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 65MN →65Mn · GB/T 1222-2016
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Spring steels
- Subcategory
- Spring steels
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 1222-2016
- Table / clause
- Table 1 · continued table · Notes a/b; 6.1.1–6.1.3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.9 ~ 1.2 |
| Cr | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.35 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
Applicability and limitations
Heat analysis, mass fractions wt%; Product-analysis tolerances are assessed separately under GB/T222 and are not included in this table. ; Table 1, note b: when required by the purchaser and stated in the contract, residual Cu may be ≤0.20%; Default tabulated limit ≤0.25%. ; 6.1.2: oxygen in 40SiMnVBE is ≤0.0015%; oxygen in other alloy spring steels is ≤0.0025%; This limit is not extended to carbon spring steels. ; Unspecified elements do not mean zero; Spring-steel composition does not establish suitability for every cold-headed component; the specific process requires a separate assessment.
Verification notes
Table 1 and its footnotes, and the oxygen-content requirement in 6.1.2, were checked.65Mn · GB /T 1222-2025
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Spring steels
- Subcategory
- Spring steels
- Material form
- Reference record
- Original record status
- Historical-edition reference
- Standard edition
- GB/T 1222-2016
- Table / clause
- Table 1 · continued table · Notes a/b; 6.1.1–6.1.3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.9 ~ 1.2 |
| Cr | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.35 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
Applicability and limitations
The chemical composition currently shown is transcribed from the original GB/T 1222-2016; The original record cites GB /T 1222-2025; that original edition remains unavailable, and differences between editions have not been confirmed. Heat analysis, mass fractions wt%; Product-analysis tolerances are assessed separately under GB/T222 and are not included in this table. ; Table 1, note b: when required by the purchaser and stated in the contract, residual Cu may be ≤0.20%; Default tabulated limit ≤0.25%. ; 6.1.2: oxygen in 40SiMnVBE is ≤0.0015%; oxygen in other alloy spring steels is ≤0.0025%; This limit is not extended to carbon spring steels. ; Unspecified elements do not mean zero; Spring-steel composition does not establish suitability for every cold-headed component; the specific process requires a separate assessment.
Verification notes
The chemical composition currently shown is transcribed from the original GB/T 1222-2016; The original record cites GB /T 1222-2025; that original edition remains unavailable, and differences between editions have not been confirmed.65Mn · GB/T 699-1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Quality carbon structural steel (source classification)
- Original record status
- Original standard verified
- Standard edition
- GB/T 699-1999
- Table / clause
- Main-text Table 1, row 30, Table 2 and Clause 6.1.1
- PDF page references
- 5、6
- Unit
- Mass fraction (%)
- Analysis type
- Ladle analysis
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.9 ~ 1.2 |
| Cr | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
Applicability and limitations
Edition 1999, main-text Table 1, row 30, unified numerical designation U21652. This record uses the default quality-steel class; heat analysis, mass fraction %. Table 2: for quality steel, P and S are each ≤0.035%; for higher-quality class A, each is ≤0.030%; for special-quality class E, the requirements are P≤0.025% and S≤0.020%. Do not apply A/E limits to the default class. 6.1.1.2—3: scrap-based steelmaking may permit Cu≤0.30%; steel for hot pressure working requires Cu≤0.20%. This record retains the default Cu≤0.25% in Table 1; specific conditions require separate confirmation. 6.1.1.4: Mn/Cr/Ni/Cu for lead-patented steel wire 35—85 has a separate restriction and does not apply to this default structural-steel record. Mechanical properties in Table 3 and 6.4 depend on specimens, dimensions, heat treatment and order requirements. Existing reference properties are not upgraded to universal guarantees by this composition review.
Verification notes
1999 original Tables 1/2 and clause 6.1.1 checked line by line.65Mn · GB/T 699-2015
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Quality carbon structural steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 699-2015
- Table / clause
- Table 1 and notes a and b; clauses 6.1.2 and 6.1.3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.9 ~ 1.2 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Cr | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
Table 1 of GB/T699-2015 gives heat-analysis mass fractions wt%; Product-analysis tolerances are listed separately under GB/T222. ; Table 1, note a: Cu≤0.20% for steel intended for hot pressure working; other tabulated cases are ≤0.25%. ; 6.1.2: N≤0.008% applies to basic oxygen steelmaking; analysis may be omitted if the supplier guarantees compliance; Applicability depends on the steelmaking method. ; 6.1.3: for lead-bath-patented wire, Mn0.30–0.60% for 35–85 and Mn0.70–1.00% for 65Mn/70Mn, Cr≤0.10/Ni≤0.15/Cu≤0.20%; P/S follows the corresponding wire standard and must not exceed Table 1. This is a conditional exception, not a general range. ; Elements not specified in the table must not be intentionally added without purchaser consent.
Verification notes
Table 1 and applicable clauses verified65Mn · GB/T 3078-2019
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Quality carbon structural steel
- Material form
- Cold-drawn bars
- Original record status
- Original standard verified
- Standard edition
- GB/T 3078-2019
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.9 ~ 1.2 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Cr | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
GB/T3078-2019, Clause 7.1.1: Quality carbon structural steel refers to GB/T699; alloy structural steel refers to GB/T3077.; The source of chemical composition must simultaneously display the referenced standard. ; Applies to cold-drawn steel bars and cold-drawn polished round bars.; Apply product-analysis tolerances under GB/T222 separately; do not incorporate them directly into heat-analysis ranges.. ; GB/T699-2015 Table 1: Cu≤0.20% for steel intended for hot working; this must not be mixed with the ordinary Cu≤0.25% limit.. ; For steel smelted by basic oxygen furnace, N≤0.008%; smelting method conditions must be specified. ; For grades 35–85 and 65Mn/70Mn used for lead-bath-patented wire, Mn, Cr, Ni and Cu are subject to the separate limits in Clause 6.1.3.; This record is for 3078 cold-drawn bar products, and does not automatically apply wire special cases.
Verification notes
The cited clauses in 3078 and the original texts of the referenced standards have been checked.Hardness in the delivery condition (conditions shown separately)
GB/T 3078-2019 · Table 2 hardness in delivery condition and Note a; 7.3/7.4 · PDF pages 6, 7 · HBW
Standard condition data, not actual measured results of supplied heats; Actual delivery condition, application, and contract must be confirmed.
- Clause 7.3.1: The specific delivery condition shall be stated in the contract; if it is not specified, delivery shall be in the cold-drawn condition.
- 7.4.1 Hardness for delivery in the normalized condition shall be agreed by both parties; the two general-use columns in Table 2 do not apply to the normalized condition.
- Values in parentheses are for reference and are not acceptance criteria.
- 7.4.2 Hot-pressure-working applications are subject to separate limits; do not automatically apply the general condition in Table 2.
- 7.4.2 For hot-pressure working, supplied in the cold-drawn condition: 50Mn2, 35CrMnSi, 42CrMo and 35CrMoV per Table 2; 38CrSi and 38CrMoAl ≤285 HBW; other grades ≤269 HBW. Confirm the actual use; the ordinary Table 2 condition cannot replace this condition.
- 7.4.3 No hardness test is performed when the nominal cross-sectional dimension (diameter, thickness or diagonal length) is below 5 mm. At the purchaser’s request, stated in the contract, tensile strength may be used instead of hardness; the specific requirements shall be agreed by both parties. This clause provides no automatic conversion relationship.
Cold-drawn or cold-drawn and bright-polished delivery; Table 2 conditions are for general use. For hot-pressure-working applications, check clause 7.4.2 separately.
Reference values in parentheses in the original table shall not be used as a basis for judgment: HBW ≤ 285 (lower limit not listed) HBW
Delivery in the annealed, bright-annealed, high-temperature-tempered or tempered-after-normalizing condition; delivery as-normalized is excluded and shall be agreed by both parties under 7.4.1.
HBW:≤ 269 (lower limit not stated) HBW
65Mn · GB /T 1222-2007
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Cr | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Mn | 0.9 ~ 1.2 |
| Ni | ≤ 0.25 (lower limit not stated) |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | 0.17 ~ 0.37 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
65Mn · GB /T 4358-1995
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.69 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.15 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | 0.17 ~ 0.37 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
65Mn · GB /T 711-2017
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Cr | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Mn | 0.9 ~ 1.2 |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | 0.17 ~ 0.37 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
65Mn · Q/ASB 84-2019
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Tool steels
- Subcategory
- Tool steels
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.65 ~ 0.7 |
| Cr | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Mn | 0.9 ~ 1.2 |
| Ni | ≤ 0.25 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | 0.17 ~ 0.37 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
65Mn · YB /T 5058-2005
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Cr | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Mn | 0.9 ~ 1.2 |
| Ni | ≤ 0.25 (lower limit not stated) |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | 0.17 ~ 0.37 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
65Mn · YB /T 5319-2010
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.62 ~ 0.7 |
| Cr | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Mn | 0.9 ~ 1.2 |
| Ni | ≤ 0.25 (lower limit not stated) |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | 0.17 ~ 0.37 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.