632 · ASTM A564/A564M-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Precipitation-hardening stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al0.75 ~ 1.5
C≤ 0.09 (lower limit not stated)
Cr14 ~ 16
Mn≤ 1 (lower limit not stated)
Mo2 ~ 3
Ni6.5 ~ 7.75
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

632 · ASTM A693-2013

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Precipitation-hardening stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al0.75 ~ 1.5
C≤ 0.09 (lower limit not stated)
Cr14 ~ 16
Mn≤ 1 (lower limit not stated)
Mo2 ~ 3
Ni6.5 ~ 7.7
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

632 · ASTM A693-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Precipitation-hardening stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al0.75 ~ 1.5
C≤ 0.09 (lower limit not stated)
Cr14 ~ 16
Mn≤ 1 (lower limit not stated)
Mo2 ~ 3
Ni6.5 ~ 7.7
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

632 · ASTM A705/A705M-2023

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Precipitation-hardening stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al0.75 ~ 1.5
C≤ 0.09 (lower limit not stated)
Cr14 ~ 16
Mn≤ 1 (lower limit not stated)
Mo2 ~ 3
Ni6.5 ~ 7.75
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

632 · ASTM A959-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Precipitation-hardening stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al0.75 ~ 1.5
C≤ 0.09 (lower limit not stated)
Cr14 ~ 16
Mn≤ 1 (lower limit not stated)
Mo2 ~ 3
Ni6.5 ~ 7.7
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations