← BackMaterial grade directory

5754

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 5754 →

5754 · GB/T 3190—1996

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Aluminum and aluminum alloys
Subcategory
Aluminum and aluminum alloys
Material form
Reference record
Original record status
Original-standard record
Standard edition
GB/T 3190—1996
Table / clause
Table 1; Clause 4.1~4.5 · Footnotes
PDF page references
3、10、13

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Si≤ 0.4 (lower limit not stated)
Fe≤ 0.4 (lower limit not stated)
Cu≤ 0.1 (lower limit not stated)
Mn≤ 0.5 (lower limit not stated)
Mg2.6 ~ 3.6
Cr≤ 0.3 (lower limit not stated)
Zn≤ 0.2 (lower limit not stated)
Ti≤ 0.15 (lower limit not stated)

Applicability and limitations

GB/T 3190—1996, Table 1, mass fraction %; unspecified elements are not treated as zero. This standard specifies the chemical composition of wrought aluminium and aluminium alloys; it does not automatically establish cold-heading suitability, actual supply, or finished-product performance. Al is the balance; the original table gives no independent numerical range for Al. Individual and total limits for other impurities apply only to the other elements referred to in clause 4.3, not to the sum of all principal alloying elements; a missing impurity test is not zero.

Combined limits

Combined-element limits
  • Requirement
    Mn+Cr (GB/T 3190—1996, Table 1)
    Element coefficient
    Mn
    1
    Cr
    1
    Lower limit
    0.1
    Upper limit
    0.6
Elements requiring measured values from the same heat
    Other-impurity requirements in the source
    Each other impurity
    0.05
    Sum of other impurities
    0.15
    Other impurities require technical review
    Yes

    5754 · JIS H 4040-2015

    Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

    Material form
    Reference record
    Original record status
    Original standard verified
    Standard edition
    JIS H 4040:2015
    Table / clause
    Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
    PDF page references
    16
    Unit
    Mass fraction (%)
    Analysis type
    Chemical composition (refer to the source notes for the analysis type)

    Carbon-equivalent reference

    IIW / CEV: not directly applicable to this material category
    Pcm (Ito–Bessyo): not directly applicable to this material category
    CET: not directly applicable to this material category

    Composition

    ElementComposition requirement
    Si≤ 0.4 (lower limit not stated)
    Fe≤ 0.4 (lower limit not stated)
    Cu≤ 0.1 (lower limit not stated)
    Mn≤ 0.5 (lower limit not stated)
    Mg2.6 ~ 3.6
    Cr≤ 0.3 (lower limit not stated)
    Zn≤ 0.2 (lower limit not stated)
    Ti≤ 0.15 (lower limit not stated)

    Applicability and limitations

    Table 2 coupled limit: Mn+Cr0.10-0.60 (mass percent); this must be satisfied together with all individual limits. ; Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable forms: extruded bars and cold-drawn bars; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.

    Verification notes

    2015: Tables 1 and 2 in the original English edition corrected page by page and cell by cell; alloy designation 5754; original PDF page 16, Table 2

    5754 · JIS H 4040-2006

    Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

    Material form
    Reference record
    Original record status
    Original standard verified
    Standard edition
    JIS H 4040:2006
    Table / clause
    Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
    PDF page references
    8
    Unit
    Mass fraction (%)
    Analysis type
    Chemical composition (refer to the source notes for the analysis type)

    Carbon-equivalent reference

    IIW / CEV: not directly applicable to this material category
    Pcm (Ito–Bessyo): not directly applicable to this material category
    CET: not directly applicable to this material category

    Composition

    ElementComposition requirement
    Si≤ 0.4 (lower limit not stated)
    Fe≤ 0.4 (lower limit not stated)
    Cu≤ 0.1 (lower limit not stated)
    Mn≤ 0.5 (lower limit not stated)
    Mg2.6 ~ 3.6
    Cr≤ 0.3 (lower limit not stated)
    Zn≤ 0.2 (lower limit not stated)
    Ti≤ 0.15 (lower limit not stated)

    Applicability and limitations

    Table 2 coupled limit: Mn+Cr0.10-0.60 (mass percent); this must be satisfied together with all individual limits. ; Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable form: cold-drawn bars; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.

    Verification notes

    2006: Tables 1 and 2 in the original Japanese edition corrected page by page and cell by cell; alloy designation 5754; original PDF page 8, Table 2
    WhatsApp Technical enquiry →