51B60 · SAE J404-2009

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J404-2009
Table / clause
Table 1 and Notes 1–7
PDF page references
1、3、4

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 1 default composition
IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6400–0.7873Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Typical P/S limits for flat products by mutual agreement
IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6400–0.7873Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Typical P/S limits for ASTM long products by mutual agreement
IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6400–0.7873Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1
Si0.15 ~ 0.35
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
Cr0.7 ~ 0.9
Mo≤ 0.06 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
B0.0005 ~ 0.003

Applicability and limitations

Original SAE 51B60 corresponds to UNS G51601; UNS is retained only as a search alias. ; Heat analysis wt%; Residual Cu≤.35%, Ni≤.25%, Cr≤.20% and Mo≤.06% are unspecified; explicit alloy ranges take precedence. ; Default and agreed P/S conditions are retained separately; Product-analysis tolerances under J409 require separate verification. ; Other Si ranges require agreement; Addition of Pb requires the L designation; ordinary grades do not include Pb. ; Required reporting of elements and reporting thresholds does not establish universal content requirements or zero content. ; Composition alone does not establish cold-heading suitability or supply availability. ; Note 3, boron range .0005–.003%.

Original condition-branch records

Table 1 default composition

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1
Si0.15 ~ 0.35
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
Cr0.7 ~ 0.9
Mo≤ 0.06 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
B0.0005 ~ 0.003

Typical P/S limits for flat products by mutual agreement

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1
Si0.15 ~ 0.35
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
Cr0.7 ~ 0.9
Mo≤ 0.06 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
B0.0005 ~ 0.003

Typical P/S limits for ASTM long products by mutual agreement

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1
Si0.15 ~ 0.35
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
Cr0.7 ~ 0.9
Mo≤ 0.06 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
B0.0005 ~ 0.003

A condition branch must be selected

Yes

Verification notes

All columns of Table 1 on PDF page 3 and footnotes on PDF page 4 visually checked.

51B60 · ASTM A29/A29M-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A29/A29M-2012
Table / clause
Table 2 · Notes 1–4; Footnotes A–C
PDF page references
1、5、6

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Si range listed in Table 2
IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6375–0.7723Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser specifies Si≤0.10%, note A
IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6325–0.7640Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Cr0.7 ~ 0.9
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Applicability and limitations

Heat analysis chemical composition mass fraction wt%; Apply product-analysis deviations under Table 6 separately; do not add them to heat-analysis limits.. Table 2 Note 1: Cu/Ni/Cr/Mo not specified as alloying ranges are allowed to be ≤0.35/0.25/0.20/0.06% respectively; Explicit alloy ranges shall take priority. Note A: The purchaser may specify Si≤0.10%, which shall be treated as a different condition from the Si range listed in the table, and the union of the two shall not be taken. Note 4: Pb is 0.15–0.35% only when lead-bearing steel designated L is separately specified.; Ordinary grades do not automatically include Pb. This standard provides general requirements for hot-worked bar products and cannot be used to commit to cold-heading suitability or supply based solely on chemical composition. Note C is for an expected B content of 0.0005–0.003%; If usual Ti addition is not permitted, B can be expected up to 0.005%. This is an expected description from the original text and is not a unified mandatory range for all deliveries; Fixed B limits shall not be added if specific contract conditions are not selected.

Original condition-branch records

Si range listed in Table 2

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Cr0.7 ~ 0.9
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Purchaser specifies Si≤0.10%, note A

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Cr0.7 ~ 0.9
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Table 2 and footnotes in the official 2012 original have been checked; select Si and the applicable purchasing conditions.

51B60 · SAE J404-2000

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Boron steels
Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J404-2000
Table / clause
Table 1 and notes 1–3; scope
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6400–0.7873Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
Ni≤ 0.25 (lower limit not stated)
Cr0.7 ~ 0.9
Mo≤ 0.06 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
B0.0005 ~ 0.003

Applicability and limitations

Standard dated 2000-6, Table 1; ladle analysis, mass fraction wt%.; Product analysis deviations shall be verified separately according to SAE J409, and shall not directly expand the table values. Note 1: For elements neither specified nor required in the original table, residual upper limits apply: Cu/Ni/Cr/Mo respectively ≤0.35/0.25/0.20/0.06%; Explicit alloy ranges shall take priority. Pb 0.15–0.35% must be separately specified as L-grade; it is not automatically added to ordinary grades. Al, Ti, Nb, and V must be reported regardless of whether they are specified; Values below 0.008% may be reported as <0.008%; this is a reporting threshold, not a uniform composition upper limit. Grades with E prefix are electric furnace steels, with P/S upper limits of 0.025% respectively, separated from ordinary grades. Applicable to billets, slabs, plate, wire rod and hot-rolled/cold-worked bar products, among other forms.; Chemical composition itself does not guarantee suitability for cold heading.

Verification notes

Original 2000 table rows and footnotes checked; the 50B46 issue is listed separately, and not all values are confirmed.

51B60 · Nippon Steel Wire Rods EXE203 2008.3 / SAE J404 JUN.2000

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Cat. No. EXE203 2008.3 PDF; cover copyright 2008
Document title
Nippon Steel Wire Rods
Table / clause
Printed page 12, table index 0
PDF page references
8
Unit
Mass fraction (%)
Analysis type
Heat analysis (identified as ladle analysis in the original table)
Manufacturer
NIPPON STEEL CORPORATION

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6400–0.7873Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Cr0.7 ~ 0.9
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)
B0.0005 ~ 0.003

Applicability and limitations

Nippon Steel wire rod catalogue EXE203 (2008.3 historical material), PDF p. 8

printed p. 12, SAE J404 JUN.2000. Ladle analysis (as labelled in source table). Manufacturer-range data; not a standard guaranteed value or a heat-lot test, and not a representation of our supply. Condition: Table-note residual limits Cu≤0.35, Ni≤0.25, Cr≤0.20 and Mo≤0.06 apply only to columns not specified as principal elements; for starred grades 50B46/51B60, B is 0.0005–0.0030%.

Composition conditions

Verification notes

Grouped tables were expanded in full and checked against original images and notes. Ordinary, residual and conditional elements are kept separate; suffix tables lacking complete base-steel composition are excluded.

51B60 · CHINA STEEL CORPORATION · Bars and Wire Rods Product Catalogue 2014-C1 / 7.1.16 SAE · Alloy steels (Edition unspecified)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Bars and wire rod
Original record status
Manufacturer source verified
Document edition
CAT.NO.3-BD-01-2014-C1 (stated on the back cover)
Document title
Bars and Wire Rods Product Catalogue
Table / clause
7.1.16 SAE · Alloy steels (Edition unspecified)
PDF page references
23
Unit
Mass fraction (%)
Analysis type
The original catalogue does not explicitly identify the analysis type for this table
Manufacturer
CHINA STEEL CORPORATION

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6400–0.7873Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.03 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Cr0.7 ~ 0.9
B0.0005 ~ 0.003
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Applicability and limitations

China Steel wire rod catalogue CAT.NO.3-BD-01-2014-C1, PDF p. 23

printed p. 21, §7.1.16 SAE alloy steels (edition not marked). The source table does not specify the analysis type. Historical manufacturer range data, not a standard-guaranteed value or heat-lot test, and not a representation of our supply. Condition: residual Cu/Ni/Cr/Mo limits supplement only elements not specified in the main table; they do not override principal alloy ranges.

Composition conditions

Verification notes

Merged cells in all 28 catalogue tables were reconstructed geometrically, with no missing cells. Original images, continuation pages and notes are recorded; disputed conditions are withheld.

51B60 · ASTM A29/A29M-2023

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A29/A29M-2023
Table / clause
Table 2 · Notes 1–4; Footnotes A–C
PDF page references
7
Unit
Mass fraction (wt%)
Analysis type
Heat analysis (composition ranges and limits in the original table)

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Si range listed in Table 2
IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6375–0.7723Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser specifies Si≤0.10%, Table 2 note A
IIW / CEV:0.8250–1.0387Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6325–0.7640Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6700–0.8147 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Cr0.7 ~ 0.9
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Applicability and limitations

Original ASTM A29/A29M-2023, Table 2: the basic table gives heat-analysis mass fractions wt%; Product-analysis tolerances require separate confirmation under 4.3 and Table 6 and are not added to heat-analysis limits. When 4.1.1 is ordered by a grade in this table, the corresponding heat-analysis limits must be met; Other ordered compositions require separate agreement under 4.1.2 and Table 3/4 and are not merged into this table. General requirements for hot-worked bars; chemistry alone does not establish cold-heading suitability, supply or mechanical properties. Table 2 Note 1: For elements where no alloy range is specified, the residual upper limits for Cu/Ni/Cr/Mo are 0.35/0.25/0.20/0.06% respectively; The alloy range specified in this row shall take priority. Table 2, Note A: The purchaser may specify Si≤0.10%; select this condition separately from the Si range in this row, without combining their ranges.. Table 2 Note 4: When L lead-bearing grades are separately specified, Pb is 0.15–0.35%; When lead is added to the ladle stream, its cast/heat-analysis content cannot be determined; do not automatically create lead-bearing grade records or add lead to ordinary-grade compositions.. Table 2 Note C: expected B 0.0005–0.003%; Where the usual Ti addition is not permitted, the expected maximum is 0.005%.. In the absence of determined contract conditions, a uniform mandatory B limit shall not be fabricated; Unlisted B shall not be assumed as zero.

Original condition-branch records

Si range listed in Table 2

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Cr0.7 ~ 0.9
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Purchaser specifies Si≤0.10%, Table 2 note A

ElementComposition requirement
C0.56 ~ 0.64
Mn0.75 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Cr0.7 ~ 0.9
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Existing OCR of the four-page, 190-row original 2023 table was parsed cell by cell. All values were screened for differences against independent 2012 data and checked against the original 2023 images and footnotes; no values were filled from the older edition.