← BackMaterial grade directory

5056

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 5056 →

5056 · GB/T 3190—1996

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Aluminum and aluminum alloys
Subcategory
Aluminum and aluminum alloys
Material form
Reference record
Original record status
Original-standard record
Standard edition
GB/T 3190—1996
Table / clause
Table 1; Clause 4.1~4.5 · Footnotes
PDF page references
3、10、13

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Si≤ 0.3 (lower limit not stated)
Fe≤ 0.4 (lower limit not stated)
Cu≤ 0.1 (lower limit not stated)
Mn0.05 ~ 0.2
Mg4.5 ~ 5.6
Cr0.05 ~ 0.2
Zn≤ 0.1 (lower limit not stated)

Applicability and limitations

GB/T 3190—1996, Table 1, mass fraction %; unspecified elements are not treated as zero. This standard specifies the chemical composition of wrought aluminium and aluminium alloys; it does not automatically establish cold-heading suitability, actual supply, or finished-product performance. Al is the balance; the original table gives no independent numerical range for Al. Individual and total limits for other impurities apply only to the other elements referred to in clause 4.3, not to the sum of all principal alloying elements; a missing impurity test is not zero.

Combined limits

Other-impurity requirements in the source
Each other impurity
0.05
Sum of other impurities
0.15
Other impurities require technical review
Yes

5056 · JIS H 4040-2015

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
JIS H 4040:2015
Table / clause
Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
PDF page references
16
Unit
Mass fraction (%)
Analysis type
Chemical composition (refer to the source notes for the analysis type)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Si≤ 0.3 (lower limit not stated)
Fe≤ 0.4 (lower limit not stated)
Cu≤ 0.1 (lower limit not stated)
Mn0.05 ~ 0.2
Mg4.5 ~ 5.6
Cr0.05 ~ 0.2
Zn≤ 0.1 (lower limit not stated)

Applicability and limitations

Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable forms: extruded bars, cold-drawn bars and cold-drawn wire; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.

Verification notes

2015: Tables 1 and 2 in the original English edition corrected page by page and cell by cell; alloy designation 5056; original PDF page 16, Table 2

5056 · JIS H 4040-2006

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
JIS H 4040:2006
Table / clause
Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
PDF page references
9
Unit
Mass fraction (%)
Analysis type
Chemical composition (refer to the source notes for the analysis type)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Si≤ 0.3 (lower limit not stated)
Fe≤ 0.4 (lower limit not stated)
Cu≤ 0.1 (lower limit not stated)
Mn0.05 ~ 0.2
Mg4.5 ~ 5.6
Cr0.05 ~ 0.2
Zn≤ 0.1 (lower limit not stated)

Applicability and limitations

Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable forms: extruded bars, cold-drawn bars and cold-drawn wire; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.

Verification notes

2006: Tables 1 and 2 in the original Japanese edition corrected page by page and cell by cell; alloy designation 5056; original PDF page 9, Table 2
WhatsApp Technical enquiry →