← BackMaterial grade directory

46MNVS3

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 46MNVS3 →

46MnVS3 · EN 10267-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Precipitation-hardening ferritic-pearlitic steel
Material form
Semi-finished products and bars for hot working; select delivery condition +U, +S or +P and verify against Table 1
Original record status
Original standard verified
Standard edition
EN 10267:1998
Table / clause
Table 3 and footnotes 1–4; Table 1 applicability
PDF page references
1、7、9
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV:0.5360–0.7727Known-element contribution; incomplete value; missing Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4630–0.6070Known-element contribution; incomplete value; missing Cu, Ni, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4800–0.6130Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.42 ~ 0.49
Si0.15 ~ 0.8
Mn0.6 ~ 1.0
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.06
N0.01 ~ 0.02
Cr≤ 0.3 (lower limit not stated)
Mo≤ 0.08 (lower limit not stated)
V0.08 ~ 0.2

Applicability and limitations

Table 3 of EN 10267:1998 is heat analysis mass fraction wt%. ; Table 1: Table 3 and Table 4 are used for untreated +U and cold-sheared +S deliveries; The chemical composition in Table 5 for precipitation hardening +P machined bars is for guidance only; Table 3 shall not be automatically regarded as a +P delivery guarantee. ; Table 3 Footnote 2: Other elements for improving machinability or controlling sulfides/oxides, as well as adjustments to the sulfur range, shall be by agreement. ; Table 3 Footnote 3: Partial or total substitution of V by Nb requires agreement; the lower limit of V must also be separately negotiated; Current composition reverse-checks shall only use the default limits of Table 3 without substitutions. ; Table 3 Footnote 4: Ti addition shall be by agreement; Elements not listed shall not be intentionally added without the buyer's consent (except additions needed to finish steelmaking). ; Product analysis deviations in Table 4 shall be verified separately; The +P mechanical properties in Table 5 correspond only to machined bars and 30–120mm; other sizes shall be by agreement; Cold-heading suitability shall be verified separately.

Verification notes

EN 10267:1998, Table 3, row 5, and Table 1 / footnotes were checked item by item; Composition in the +P condition is for guidance only.

46MnVS3 · Ovako Product Catalogue CO-117 ENG 24:07 (2024)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Bars, tubes, rings and precomponents
Composition basis
Manufacturer typical/nominal values, not guaranteed ranges
Original record status
Manufacturer source verified
Document edition
CO-117 ENG 24:07 ©Ovako 2024
Document title
Ovako Product Catalogue
PDF page references
44
Unit
Interpreted as mass fraction (%) using other documents from the same manufacturer; the unit is not explicitly stated in this table
Analysis type
Typical composition analysis
Manufacturer
Ovako

Source document

Carbon-equivalent reference

Manufacturer typical single values are composition references only; no range estimate is made. They are neither standard guarantees nor measured heat results; Formula applicability requires review against the intended use and process.

IIW / CEV: manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated
CET: manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
CTypical/nominal value 0.46 (not a guaranteed range)
SiTypical/nominal value 0.3 (not a guaranteed range)
MnTypical/nominal value 0.7 (not a guaranteed range)

Applicability and limitations

Ovako 2024 product catalogue, PDF page 44; manufacturer’s typical analysis, for composition reference only. The original header does not explicitly state units; interpreted using the manufacturer’s mass-fraction % information. Neither standard guaranteed values nor measured heat analysis. Excluded from limit-based reverse search and carbon-equivalent calculation; blanks and element names alone in the other-elements field are not filled with 0. Manufacturer code: 382.

Conditional requirement

Verification notes

All 170 rows of the 2021 original table were visually checked. Values in corresponding 2024 cells are unchanged; recognition differences were reviewed separately. Rows with conflicting values under the same code are excluded; values are not mixed across sections.

Source notes

Micro-alloyed high strength steel suitable for surface induction hardening

Other-element requirements

V
WhatsApp Technical enquiry →