← BackMaterial grade directory

4621H

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 4621H →

4621H · ASTM A304-2020

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Structural steel with guaranteed hardenability
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A304-2020
Table / clause
Table 1 · Footnotes; 1.1–1.2, 7.1
PDF page references
1、2、3、5

Source document

Carbon-equivalent reference

IIW / CEV:0.4133–0.6533Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2442–0.3725Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2888–0.4375 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.17 ~ 0.23
Mn0.6 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.15 ~ 0.35
Ni1.55 ~ 2.0
Mo0.2 ~ 0.3
Cu≤ 0.35 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)

Applicability and limitations

ASTM A304—2020 Tables 1 and 2 and 7.1 specify ladle analysis, mass fraction (wt%); this is an excerpt from the published edition, not verification of the complete standard. The scope is hot-worked carbon, alloy and carbon-boron steel bars with hardenability requirements; the H suffix must not be omitted or treated automatically as an ordinary grade. Product-analysis tolerances in Table 1 note 3 must be checked separately against A29/A29M; tolerances and hardenability bands were not reproduced here, and composition alone does not establish compliance with all H-steel requirements. Unlisted elements are not zero; residual-element maxima not specified in Table 1 note 2 are included for the applicable elements. Table 1 note 2 is not automatically applied to Table 2. A leaded variant requires the separate L designation in the source; Pb 0.15–0.35% has not been added to ordinary H grades. The boron-steel footnote states an expected minimum boron content of 0.0005%; it is listed separately and is not presented as a composition acceptance limit. Chemistry outside this table requires agreement between purchaser and supplier. Inclusion in the standard-material database does not establish cold-heading supply capability or direct substitutability; processing and supply conditions must be confirmed separately.

Verification notes

PDF pages 1/2/3/5 visually checked; composition-table rows and footnotes extracted and verified separately.