← BackMaterial grade directory

45CRNIMOV

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 45CRNIMOV →

45CrNiMoV · GB/T 3077-2015

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy structural steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 3077-2015
Table / clause
Tables 1 and 2; A/E designation rules in the endnote to Table 1

Carbon-equivalent reference

IIW / CEV:0.8100–1.0833 Independent-element envelope of standard ranges; not measured heat-analysis values CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.5357–0.6823Known-element contribution; incomplete value; missing B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.5625–0.7150 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.42 ~ 0.49
Mn0.5 ~ 0.8
Cr0.8 ~ 1.1
Mo0.2 ~ 0.3
Ni1.3 ~ 1.8
Si0.17 ~ 0.37
V0.1 ~ 0.2
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

GB/T 3077-2015 Table 1 gives ladle analysis; Table 2 gives P/S and residual-element requirements. The final note to Table 1 allows ordering any grade as higher or special quality by adding A or E after the grade; this record is ordinary quality steel. For steel used in hot-pressure working, Cu ≤0.20%; the ordinary Cu maximum does not apply to this use. Explicit alloy ranges in Table 1 take priority; for Cr/Ni/Mo not specified there, use the residual limits in Table 2 and do not add residual limits on top of alloying-element ranges. Sn/Sb/As must be analyzed and recorded on the inspection certificate; any needed limits require agreement, and no generic numerical limits are invented here. Product-analysis deviations are handled separately under GB/T 222 and do not directly expand ladle limits. Mechanical properties depend on specimen dimensions and the recommended heat-treatment/delivery condition; this composition review does not constitute verification of properties.

Verification notes

Tables 1/2 and quality-grade rules checked

45CrNiMoV · GB/T 3078-2019

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy structural steel
Material form
Cold-drawn bars
Original record status
Original standard verified
Standard edition
GB/T 3078-2019

Carbon-equivalent reference

IIW / CEV:0.8100–1.0833 Independent-element envelope of standard ranges; not measured heat-analysis values CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.5357–0.6823Known-element contribution; incomplete value; missing B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.5625–0.7150 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.42 ~ 0.49
Mn0.5 ~ 0.8
Cr0.8 ~ 1.1
Mo0.2 ~ 0.3
Ni1.3 ~ 1.8
Si0.17 ~ 0.37
V0.1 ~ 0.2
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

Clause 7.1.1 of GB/T3078—2019: quality carbon structural steels comply with GB/T699, and alloy structural steels with GB/T3077; the referenced composition standard must also be displayed. This grade is listed in row 71 of Table 2. Hardness for each delivery condition is listed separately under Table 2; the actual application and delivery condition require separate verification and are not assumed to comply. Cold-drawn steel bars/cold-drawn polished round bars: product-analysis deviations under GB/T222 require separate verification and are not added to heat-analysis ranges. In GB/T3077-2015, Table 1 gives heat analysis and Table 2 gives P/S and residual-element requirements. The final note to Table 1 permits all grades to be ordered as higher or special quality, with the respective suffixes A/E; this record uses the default quality-steel class. Steel for hot pressure working: Cu≤0.20%; the ordinary Cu upper limit does not apply to that use. Explicit alloy ranges in Table 1 take precedence. Where Cr/Ni/Mo is not explicitly specified, the residual limits in Table 2 apply; residual limits are not added to specified alloy-element ranges. Sn/Sb/As must be analysed and recorded on the inspection certificate, with limits agreed where needed; no universal numerical limit is invented here. Product-analysis deviations under GB/T222 are used separately and do not directly widen heat-analysis ranges. Mechanical properties depend on specimen dimensions and the recommended heat-treatment/delivery conditions; this composition review does not establish verification of mechanical properties.

Verification notes

GB/T 3078-2019 Table 2 grade rows and the clause 7.1.1 reference checked; composition comes from the verified GB/T 3077-2015 original, not a separate composition table in GB/T 3078.

Hardness in the delivery condition (conditions shown separately)

GB/T 3078-2019 · Table 2 hardness in delivery condition and Note a; 7.3/7.4 · PDF pages 6, 7 · HBW

Standard condition data, not actual measured results of supplied heats; Actual delivery condition, application, and contract must be confirmed.

Cold-drawn or cold-drawn and bright-polished delivery; Table 2 conditions are for general use. For hot-pressure-working applications, check clause 7.4.2 separately.

Reference values in parentheses in the original table shall not be used as a basis for judgment: HBW ≤ 285 (lower limit not listed) HBW

Delivery in the annealed, bright-annealed, high-temperature-tempered or tempered-after-normalizing condition; delivery as-normalized is excluded and shall be agreed by both parties under 7.4.1.

HBW:≤ 269 (lower limit not stated) HBW