← BackMaterial grade directory

42CRNI2SI2MOVA

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 42CRNI2SI2MOVA →

42CrNi2Si2MoVA · GB/T 38809-2020

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 38809-2020
Table / clause
Table 2 and notes a/b and 5.1.1
PDF page references
1、5

Carbon-equivalent reference

IIW / CEV:0.8200–1.0567 Independent-element envelope of standard ranges; not measured heat-analysis values CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.5658–0.6892Known-element contribution; incomplete value; missing B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.5663–0.6975 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.4 ~ 0.45
Si1.45 ~ 1.8
Mn0.6 ~ 0.9
P≤ 0.01 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Cr0.7 ~ 0.95
Ni1.65 ~ 2.0
Mo0.3 ~ 0.5
V0.05 ~ 0.1
Cu≤ 0.2 (lower limit not stated)

Applicability and limitations

Official GB/T38809-2020 cover PDF1, PDF5 Table 2 and footnote a/b, heat-analysis mass fractions wt%. ; Product-analysis tolerances follow Table 3 and GB/T222 separately; they are not added to the default heat-analysis range. ; Steel-bar application, steelmaking, delivery condition, specimen heat treatment and mechanical requirements must be confirmed separately; This does not automatically establish a cold-heading product or supply guarantee.

Verification notes

The cover, all 7 grades in Table 2 and footnotes in the official original text were visually checked