40CRNI2SI2MOVA
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 40CRNI2SI2MOVA →40CrNi2Si2MoVA · GB/T 38809-2020
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 38809-2020
- Table / clause
- Table 2 and notes a/b and 5.1.1
- PDF page references
- 1、5
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.38 ~ 0.43 |
| Si | 1.45 ~ 1.8 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.01 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Cr | 0.7 ~ 0.95 |
| Ni | 1.65 ~ 2.0 |
| Mo | 0.3 ~ 0.5 |
| V | 0.05 ~ 0.1 |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Official GB/T38809-2020 cover PDF1, PDF5 Table 2 and footnote a/b, heat-analysis mass fractions wt%. ; Product-analysis tolerances follow Table 3 and GB/T222 separately; they are not added to the default heat-analysis range. ; Steel-bar application, steelmaking, delivery condition, specimen heat treatment and mechanical requirements must be confirmed separately; This does not automatically establish a cold-heading product or supply guarantee.