40CrH · GB/T 5216-2004

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5216-2004
Table / clause
Tables 1 and 2, notes a–c and clause 6.1; 15CrMoH includes Amendment No. 1
PDF page references
1、6、7

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Tables 1/2: default heat analysis
IIW / CEV:0.5933–0.8417Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5698Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6025Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H
IIW / CEV:0.5933–0.8417Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5698Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6025Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Hot pressure working Cu≤.20%
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
For hot-pressure working, Cu≤0.20%; if the purchaser requires semi-free-cutting S at 0.020–0.035%, prefix the designation H with S.
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Applicability and limitations

GB/T 5216—2004 original Tables 1/2 and 6.1, ladle-analysis mass fraction wt%; retain the actual 2004 edition.

For high-quality steel, Note a to Table 1 adds A before H (e.g. 40CrAH); P/S by quality level and residual Cu/Cr/Ni follow Table 2; do not mix with the 2014 edition.

Under 6.1.3, Cu≤0.20% for hot-pressure processing. If the purchaser requires S 0.020–0.035%, add S before H; the sulfur tolerance ±0.005 is separately stated and does not expand the default range.

Table 1 alloy-element ranges take precedence over Table 2 residual limits; a blank means unspecified, not zero.

H/HH/HL hardenability bands, delivery condition, hardness and suitability for cold-heading processes require separate verification; this does not automatically create a supply product.

Original condition-branch records

Tables 1/2: default heat analysis

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Hot pressure working Cu≤.20%

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

For hot-pressure working, Cu≤0.20%; if the purchaser requires semi-free-cutting S at 0.020–0.035%, prefix the designation H with S.

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

2004 original: all 24 rows, Table 2 and Amendment No. 1 visually checked; high-quality grade applied according to note a.

40CrH · GB/T 5216-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5216-2014
Table / clause
Table 1 and notes a/b; clauses 6.1.1–6.1.4
PDF page references
1、7、8

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Typically, residual Cu ≤0.25%; default S ≤0.035%
IIW / CEV:0.5933–0.8383Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5673Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6000Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Normally residual Cu ≤0.25%; at the purchaser’s request, S is 0.015–0.035% (the ±0.005% product-analysis tolerance for S must be checked separately).
IIW / CEV:0.5933–0.8383Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5673Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6000Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
For hot-pressure working, Cu≤0.20%; default S≤0.035%.
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
For hot-pressure working, Cu≤0.20%; S 0.015–0.035% only when required by the purchaser (product-analysis tolerance ±0.005 to be checked separately).
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Applicability and limitations

Official GB/T5216-2014, cover PDF1, Clause 6.1 PDF7, Table 1 and footnotes PDF8/9; Heat-analysis mass fractions wt%. ; Clause 6.1.2 residual Cu≤.25, Cr≤.30, Ni≤.30%; Specified alloy ranges in the table shall take priority; Hot working Cu≤.20 separate condition. ; 6.1.3 O≤.0020%; Unspecified residual limits such as Mo must not be assumed zero. ; Note a: Only for 16CrMnH/20CrMnH/25CrH/28CrH, Si≤.12% may be agreed at the buyer's request; the effect on mechanical properties must be considered.. ; Note b: Per buyer's request, S may be .015–.035%; in this case, the finished product tolerance is ±.005%, which is not a default heat analysis relaxation. ; H/HH/HL are different hardenability bands; S denotes a sulfur-related grade-designation condition.; Only compositions of H grades are listed this time; hardenability curves and all mechanical properties are not claimed to have been verified. ; The intended use for metal forming or machining under this standard must be stated in the contract.; Cold heading, annealing and actual wire-rod supply require separate confirmation; do not automatically add products..

Original condition-branch records

Typically, residual Cu ≤0.25%; default S ≤0.035%

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Normally residual Cu ≤0.25%; at the purchaser’s request, S is 0.015–0.035% (the ±0.005% product-analysis tolerance for S must be checked separately).

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S0.015 ~ 0.035
Cu≤ 0.25 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

For hot-pressure working, Cu≤0.20%; default S≤0.035%.

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

For hot-pressure working, Cu≤0.20%; S 0.015–0.035% only when required by the purchaser (product-analysis tolerance ±0.005 to be checked separately).

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S0.015 ~ 0.035
Cu≤ 0.2 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Official source cover, all 32 grades in Table 1, footnotes and 6.1 visually checked.

40CrH · GB/T 5216-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5216-2014
Table / clause
Table 1 and notes a/b; clauses 6.1.1–6.1.4
PDF page references
1、7、8

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Typically, residual Cu ≤0.25%; default S ≤0.035%
IIW / CEV:0.5933–0.8383Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5673Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6000Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Normally residual Cu ≤0.25%; at the purchaser’s request, S is 0.015–0.035% (the ±0.005% product-analysis tolerance for S must be checked separately).
IIW / CEV:0.5933–0.8383Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5673Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6000Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
For hot-pressure working, Cu≤0.20%; default S≤0.035%.
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
For hot-pressure working, Cu≤0.20%; S 0.015–0.035% only when required by the purchaser (product-analysis tolerance ±0.005 to be checked separately).
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Applicability and limitations

Official GB/T5216-2014, cover PDF1, Clause 6.1 PDF7, Table 1 and footnotes PDF8/9; Heat-analysis mass fractions wt%. ; Clause 6.1.2 residual Cu≤.25, Cr≤.30, Ni≤.30%; Specified alloy ranges in the table shall take priority; Hot working Cu≤.20 separate condition. ; 6.1.3 O≤.0020%; Unspecified residual limits such as Mo must not be assumed zero. ; Note a: Only for 16CrMnH/20CrMnH/25CrH/28CrH, Si≤.12% may be agreed at the buyer's request; the effect on mechanical properties must be considered.. ; Note b: Per buyer's request, S may be .015–.035%; in this case, the finished product tolerance is ±.005%, which is not a default heat analysis relaxation. ; H/HH/HL are different hardenability bands; S denotes a sulfur-related grade-designation condition.; Only compositions of H grades are listed this time; hardenability curves and all mechanical properties are not claimed to have been verified. ; The intended use for metal forming or machining under this standard must be stated in the contract.; Cold heading, annealing and actual wire-rod supply require separate confirmation; do not automatically add products..

Original condition-branch records

Typically, residual Cu ≤0.25%; default S ≤0.035%

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Normally residual Cu ≤0.25%; at the purchaser’s request, S is 0.015–0.035% (the ±0.005% product-analysis tolerance for S must be checked separately).

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S0.015 ~ 0.035
Cu≤ 0.25 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

For hot-pressure working, Cu≤0.20%; default S≤0.035%.

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

For hot-pressure working, Cu≤0.20%; S 0.015–0.035% only when required by the purchaser (product-analysis tolerance ±0.005 to be checked separately).

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.03 (lower limit not stated)
S0.015 ~ 0.035
Cu≤ 0.2 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Official source cover, all 32 grades in Table 1, footnotes and 6.1 visually checked.

40CrH · GB/T 5216-2004

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5216-2004
Table / clause
Tables 1 and 2, notes a–c and clause 6.1; 15CrMoH includes Amendment No. 1
PDF page references
1、6、7

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Tables 1/2: default heat analysis
IIW / CEV:0.5933–0.8417Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5698Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6025Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H
IIW / CEV:0.5933–0.8417Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5698Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.6025Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Hot pressure working Cu≤.20%
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
For hot-pressure working, Cu≤0.20%; if the purchaser requires semi-free-cutting S at 0.020–0.035%, prefix the designation H with S.
IIW / CEV:0.5933–0.8350Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4357–0.5648Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4550–0.5975Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Applicability and limitations

GB/T 5216—2004 original Tables 1/2 and 6.1, ladle-analysis mass fraction wt%; retain the actual 2004 edition.

For high-quality steel, Note a to Table 1 adds A before H (e.g. 40CrAH); P/S by quality level and residual Cu/Cr/Ni follow Table 2; do not mix with the 2014 edition.

Under 6.1.3, Cu≤0.20% for hot-pressure processing. If the purchaser requires S 0.020–0.035%, add S before H; the sulfur tolerance ±0.005 is separately stated and does not expand the default range.

Table 1 alloy-element ranges take precedence over Table 2 residual limits; a blank means unspecified, not zero.

H/HH/HL hardenability bands, delivery condition, hardness and suitability for cold-heading processes require separate verification; this does not automatically create a supply product.

Original condition-branch records

Tables 1/2: default heat analysis

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Hot pressure working Cu≤.20%

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

For hot-pressure working, Cu≤0.20%; if the purchaser requires semi-free-cutting S at 0.020–0.035%, prefix the designation H with S.

ElementComposition requirement
C0.37 ~ 0.44
Si0.17 ~ 0.37
Mn0.5 ~ 0.85
Cr0.7 ~ 1.1
P≤ 0.035 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

2004 original: all 24 rows, Table 2 and Amendment No. 1 visually checked; high-quality grade applied according to note a.
WhatsApp Technical enquiry →