← BackMaterial grade directory

39MNCRB6-4

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 39MNCRB6-4 →

39MnCrB6-4 · Ovako Product Catalogue CO-117 ENG 24:07 (2024)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Boron steels
Subcategory
Boron steels
Material form
Bars, tubes, rings and precomponents
Composition basis
Manufacturer typical/nominal values, not guaranteed ranges
Original record status
Manufacturer source verified
Document edition
CO-117 ENG 24:07 ©Ovako 2024
Document title
Ovako Product Catalogue
PDF page references
46
Unit
Interpreted as mass fraction (%) using other documents from the same manufacturer; the unit is not explicitly stated in this table
Analysis type
Typical composition analysis
Manufacturer
Ovako

Source document

Carbon-equivalent reference

Manufacturer typical single values are composition references only; no range estimate is made. They are neither standard guarantees nor measured heat results; Formula applicability requires review against the intended use and process.

IIW / CEV: manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated
CET: manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
CTypical/nominal value 0.39 (not a guaranteed range)
SiTypical/nominal value 0.3 (not a guaranteed range)
MnTypical/nominal value 1.5 (not a guaranteed range)
CrTypical/nominal value 0.5 (not a guaranteed range)

Applicability and limitations

Ovako 2024 product catalogue PDF, page 46; Manufacturer Typical analysis typical values, for composition reference only. The original table header does not explicitly state the unit; interpreted as manufacturer mass-percentage data; Not guaranteed standard limits or heat-specific measurements; Excluded from limit-based reverse matching and carbon-equivalent calculations; blanks and entries giving only the element name Other are not filled with 0. Manufacturer codes: BCM 414.

Conditional requirement

Verification notes

All 170 rows of the 2021 original table were visually checked. Values in corresponding 2024 cells are unchanged; recognition differences were reviewed separately. Rows with conflicting values under the same code are excluded; values are not mixed across sections.

Source notes

Boron alloyed heat treatable steel

Other-element requirements

B