← BackMaterial grade directory

38MNB5

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 38MNB5 →

38MnB5 · DIN EN 10083-3-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10083-3-2007
Table / clause
Table 3 · Notes a–c
PDF page references
1、18

Carbon-equivalent reference

IIW / CEV:0.5517–0.6617 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4215–0.5308Known-element contribution; incomplete value; missing Cu, Cr, Ni, Mo, V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4750–0.5650 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.36 ~ 0.42
Mn1.15 ~ 1.45
S≤ 0.035 (lower limit not stated)
B0.0008 ~ 0.005
Si≤ 0.4 (lower limit not stated)
P≤ 0.025 (lower limit not stated)

Applicability and limitations

Composition is based on Table 3 of EN10083-3:2006 in the official English text of DIN EN10083-3:2007-01, heat analysis wt%. ; Note a: Elements not listed shall not be intentionally added without the purchaser's consent, except for additions needed to finish steelmaking and to enable boron to act on hardenability.; Unspecified values shall not be treated as zero. ; Note b: Small deviations are permitted where hardenability or quenched-and-tempered mechanical-property requirements apply, except for C/P/S; permitted deviations for other elements must not exceed Table 4.; Default heat analysis range shall not be expanded. ; For non-boron steels in this standard, Note c permits steel with improved machinability to be supplied on request: sulfur approximately 0.10%, with the Mn upper limit permitted to increase by an absolute 0.15%.; Approximate values are not default hard upper limits and must be determined by specific inquiry/order; they shall not be automatically mixed with ordinary grades. ; This standard covers alloy steels for quenching and tempering. Suitability for cold heading, wire-rod supply, annealing, surface and dimensions require separate confirmation; do not automatically add products..

Verification notes

Official English source cover, all 28 grades in Table 3 and notes a–c visually checked.

Permitted product-analysis deviations (must not be added to heat-analysis limits)

DIN EN10083-3:2007-01 (adopting EN10083-3:2006) · Table 4 and notes a/b, 7.1.2.2; Product analysis specified at ordering follows A.5 · PDF pages 11, 19, 55 · mass fraction wt%; Deviations are expressed in percentage points of mass percentage

The complete standard tolerance table applies only to elements specified in the original table for this grade and to the corresponding content/sulfur-range conditions; it does not widen heat-analysis composition, carbon equivalent or reverse-search ranges.

ElementSpecified maximum heat-analysis content, wt%Lower deviation, percentage pointsUpper deviation, percentage pointsApplicable conditions
C≤0.55-0.02+0.02Select the cast-analysis maximum-content band specified in the original table
Si≤0.40The original table does not state a negative deviation+0.03Select the cast-analysis maximum-content band specified in the original table
Mn≤1.00-0.04+0.04Select the cast-analysis maximum-content band specified in the original table
Mn>1.00≤1.70-0.05+0.05Select the cast-analysis maximum-content band specified in the original table
P≤0.025The original table does not state a negative deviation+0.005Select the cast-analysis maximum-content band specified in the original table
S≤0.040The original table does not state a negative deviation+0.005Only the sulfur upper limit is specified; Note b’s full 0.020–0.040% range is not applied.
Cr≤2.00-0.05+0.05Select the cast-analysis maximum-content band specified in the original table
Cr>2.00≤2.20-0.1+0.1Select the cast-analysis maximum-content band specified in the original table
Mo≤0.30-0.03+0.03Select the cast-analysis maximum-content band specified in the original table
Mo>0.30≤0.60-0.04+0.04Select the cast-analysis maximum-content band specified in the original table
Ni≤2.00-0.05+0.05Select the cast-analysis maximum-content band specified in the original table
Ni>2.00≤4.3-0.07+0.07Select the cast-analysis maximum-content band specified in the original table
V≤0.25-0.02+0.02Select the cast-analysis maximum-content band specified in the original table
B≤0.0050-0.0003+0.0003Select the cast-analysis maximum-content band specified in the original table
S≤0.040-0.005+0.005Only when Table 3 heat analysis explicitly specifies the full S range of 0.020–0.040% (Table 4, Note b).

This is a complete standard deviation table and does not imply that every element for this grade is specified; Elements not listed are not added on the basis of this table. Symmetric deviation for the same heat is permitted in only one direction, either upward or downward; Asymmetric deviation for Pb is only found in the Pb row of EN10087 and cannot be applied to other standards where Pb is not listed. Do not automatically expand heat analysis composition, carbon equivalent, or reverse-lookup ranges.