← BackMaterial grade directory

35B2

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 35B2 →

35B2 · EN 10269-2013

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10269-2013
Table / clause
Table1 quenched-and-tempered steels and note a/b/c
PDF page references
17、19

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Ordinary sulfur requirement in Table 1
IIW / CEV:0.4033–0.5233 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3490–0.4683Known-element contribution; incomplete value; missing Cu, Cr, Ni, Mo, V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4700 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Agreed at enquiry or ordering to improve machinability, S .015–.030%
IIW / CEV:0.4033–0.5233 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3490–0.4683Known-element contribution; incomplete value; missing Cu, Cr, Ni, Mo, V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4700 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Welding condition agreed at enquiry or ordering, S .008–.030%
IIW / CEV:0.4033–0.5233 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3490–0.4683Known-element contribution; incomplete value; missing Cu, Cr, Ni, Mo, V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4700 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.32 ~ 0.39
Si≤ 0.4 (lower limit not stated)
Mn0.5 ~ 0.8
P≤ 0.03 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Al≥ 0.02 (upper limit not stated)
B0.0008 ~ 0.005

Applicability and limitations

EN10269:2013 Table 1, section on steels for quenching and tempering; official BS adoption in English, PDF17 and footnotes PDF19; heat analysis wt%.. ; The Al column is total aluminum; For ≥.020 without a specified upper limit, only the lower limit is retained; no upper limit shall be created. ; Note b sulfur agreement applies only to grades with Note b; 27NiCrMoV15-6 magnetic properties Note c carbon upper limit .28 selected separately. ; Elements not listed shall not be intentionally added without the consent of the purchaser, except additions needed to finish steelmaking; Blank does not represent zero. ; Product analysis deviation, mechanical properties, heat treatment, and cold-heading supply suitability shall be verified separately, and not automatically added to the product center.

Original condition-branch records

Ordinary sulfur requirement in Table 1

ElementComposition requirement
C0.32 ~ 0.39
Si≤ 0.4 (lower limit not stated)
Mn0.5 ~ 0.8
P≤ 0.03 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Al≥ 0.02 (upper limit not stated)
B0.0008 ~ 0.005

Agreed at enquiry or ordering to improve machinability, S .015–.030%

ElementComposition requirement
C0.32 ~ 0.39
Si≤ 0.4 (lower limit not stated)
Mn0.5 ~ 0.8
P≤ 0.03 (lower limit not stated)
S0.015 ~ 0.03
Al≥ 0.02 (upper limit not stated)
B0.0008 ~ 0.005

Welding condition agreed at enquiry or ordering, S .008–.030%

ElementComposition requirement
C0.32 ~ 0.39
Si≤ 0.4 (lower limit not stated)
Mn0.5 ~ 0.8
P≤ 0.03 (lower limit not stated)
S0.008 ~ 0.03
Al≥ 0.02 (upper limit not stated)
B0.0008 ~ 0.005

A condition branch must be selected

Yes

Verification notes

Quenched-and-tempered steels in official English Table 1 and the applicable footnotes were visually checked

35B2 · NF EN 10269:1999

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original-standard record
Standard edition
NF EN 10269:1999
Table / clause
EN 10269:1999 Table 1 and footnotes 1 and 2
PDF page references
2、21、23

Carbon-equivalent reference

IIW / CEV:0.4033–0.5233 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3490–0.4683Known-element contribution; incomplete value; missing Cu, Cr, Ni, Mo, V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4700 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.32 ~ 0.39
Si≤ 0.4 (lower limit not stated)
Mn0.5 ~ 0.8
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Al≥ 0.02 (upper limit not stated)
B0.0008 ~ 0.005

Applicability and limitations

The cover of NF EN 10269:1999 explicitly adopts EN 10269:1999; Preserve the correspondence between the French adoption version and the European version; do not label as other countries or new editions. ; Table 1 gives heat-analysis mass percentages; Single values in P and S columns are upper limits; other single values are parsed according to the inequality signs in the original table; Unspecified elements shall not be filled as zero. ; Applies to billets, bars and wire rod of steels and nickel alloys for fasteners with specified high- or low-temperature properties.; Cold heading and actual supply must be verified in conjunction with delivery condition, dimensions, and process. ; Table 1 Footnote 1: Elements not listed in the table shall not be intentionally added without the buyer's consent (except additions needed to finish steelmaking); Elements that affect properties must be prevented from being introduced via scrap steel, etc.. ; This record only verifies the heat analysis composition in Table 1; product analysis tolerances in Table 2 shall not be automatically added to the heat limits.

Combined limits

Combined-element limits