← BackMaterial grade directory

33SIMNB7-3

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 33SIMNB7-3 →

33SiMnB7-3 · Ovako Product Catalogue CO-117 ENG 24:07 (2024)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Spring steels
Subcategory
Spring steels
Material form
Bars, tubes, rings and precomponents
Composition basis
Manufacturer typical/nominal values, not guaranteed ranges
Original record status
Manufacturer source verified
Document edition
CO-117 ENG 24:07 ©Ovako 2024
Document title
Ovako Product Catalogue
PDF page references
42
Unit
Interpreted as mass fraction (%) using other documents from the same manufacturer; the unit is not explicitly stated in this table
Analysis type
Typical composition analysis
Manufacturer
Ovako

Source document

Carbon-equivalent reference

Manufacturer typical single values are composition references only; no range estimate is made. They are neither standard guarantees nor measured heat results; Formula applicability requires review against the intended use and process.

IIW / CEV: manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated
CET: manufacturer typical/nominal single values are shown for reference only; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
CTypical/nominal value 0.33 (not a guaranteed range)
SiTypical/nominal value 1.7 (not a guaranteed range)
MnTypical/nominal value 0.9 (not a guaranteed range)

Applicability and limitations

Ovako 2024 product catalogue PDF, page 42. Manufacturer Typical analysis typical values are composition references only. Units are not explicitly stated in the original header and are interpreted as mass fraction % from the manufacturer's documentation. These are neither standard-guaranteed values nor measured heat-analysis results. They are excluded from limit-based reverse lookup and carbon-equivalent calculations. Blank entries, and Other given only as an element name, are not assigned 0. Manufacturer code: SB33S17B.

Conditional requirement

Verification notes

All 170 rows of the 2021 original table were visually checked. Values in corresponding 2024 cells are unchanged; recognition differences were reviewed separately. Rows with conflicting values under the same code are excluded; values are not mixed across sections.

Source notes

Lean spring steel alloyed with boron

Other-element requirements

B
WhatsApp Technical enquiry →