← BackMaterial grade directory

316TI

8 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 316TI →

316Ti · Walsin Lihwa official website catalog (steel billets and bars; file named 2024, original edition not indicated)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Bars
Original record status
Manufacturer source verified
Document edition
Official website document 2024_Walsin_Catalog_YT-JY-1.pdf; Publication date and edition number not specified on inner pages
Document title
Available Stainless Steel Grades & Chemical Composition — For Stainless Steel Billet & Bar
Table / clause
Steel grades and chemical composition table
PDF page references
7
Unit
Percentages as stated in the original table; refer to the source for the specific basis
Analysis type
Analysis type not stated
Manufacturer
Walsin Lihwa

Source document

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni10.5 ~ 13.5
Cr16.5 ~ 18.0
Mo2.0 ~ 2.5
Ti≤ 0.7 (lower limit not stated)

Applicability and limitations

Walsin Lihwa official catalogue, PDF physical page 7

printed page 10, row 23; manufacturer's composition table, %, covering billets and bars. Analysis type is not stated. The official filename contains 2024, but no revision number was found inside; this is neither a verified edition of the cross-referenced standards nor a supply guarantee by our company. Condition: Ti=5*C-0.7; the minimum is coupled and the formula is not converted into a fixed numerical value.

Composition conditions

Combined limits

Combined-element limits
  • Element coefficient
    Ti
    1
    C
    -5.0
    Lower limit
    0

Verification notes

Composition, conditional rows and linked requirements checked cell by cell against the original image; anomalous row 303 on page 10 excluded.

316Ti · ASME SA-240

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
N≤ 0.1 (lower limit not stated)
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

316Ti · ASTM A 314-2025

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

316Ti · ASTM A240/A240M-2020

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
N≤ 0.1 (lower limit not stated)
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

316Ti · ASTM A554-2026

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
N≤ 0.1 (lower limit not stated)
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

316Ti · ASTM A959-2004

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
N≤ 0.1 (lower limit not stated)
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

316Ti · ASTM A959-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
N≤ 0.1 (lower limit not stated)
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

316Ti · Q/RP 007-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Cu≤ 0.75 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
N≤ 0.05 (lower limit not stated)
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →