3104

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 3104 →

3104 · GB/T 3880.1-2006

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Aluminum and aluminum alloys
Material form
Plate, sheet and strip
Original record status
Original standard verified
Standard edition
GB/T 3880.1-2006
Table / clause
4.2, Table 5 and note a/b; Clauses 1 and 2
PDF page references
3、9

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Si≤ 0.6 (lower limit not stated)
Fe≤ 0.8 (lower limit not stated)
Cu0.05 ~ 0.25
Mn0.8 ~ 1.4
Mg0.8 ~ 1.3
Zn≤ 0.25 (lower limit not stated)
Ga≤ 0.05 (lower limit not stated)
V≤ 0.05 (lower limit not stated)
Ti≤ 0.1 (lower limit not stated)

Applicability and limitations

GB/T3880.1—2006 Table 5 and 4.2, mass fraction %; Only 3102, 3104, and 8011A have compositions directly specified in this table; other grades refer to GB/T3190 and cannot be copied from this table. Applicable to rolled aluminum and aluminum alloy plate, sheet and strip for general industrial use.; The scope of this edition excludes special uses such as deep drawing, painting, anodizing, curtain walls and PS plate substrates, as well as plate, sheet and strip for military applications; it does not directly establish cold-heading wire/wire rod suitability.. Other impurities: individual ≤0.05%, total ≤0.15%, referring to metallic elements not listed or with no specified values in the table; these must be verified separately against the full set of measured values. Al is the remainder: 100% minus the sum of all metallic impurities with content ≥0.010%; each element shall be expressed to 0.0X% before summation; Elements with no given values must not be assumed as zero for calculation. Use for food applications must be specified in the contract, with Pb, Sn and Sb each ≤0.01%.; The conditions for this use require separate verification; food-application limits are not imposed on all industrial materials.. The chemical table and scope have been verified in this instance; this does not imply that mechanical properties, dimensions, states of all grades, or the 2012 edition have been verified.

Combined limits

Other-impurity requirements in the source
Each other impurity
0.05
Sum of other impurities
0.15
Other impurities require technical review
Yes
Source-specified balance calculation
Element
Al
Applicable rule
100% minus the sum of all metallic impurities with contents ≥0.010%; Express to 0.0X% before summation
The balance requires technical verification
Yes

Verification notes

The scope on pages 3 and 9, all three rows of Table 5 and note a/b in original PDF were visually checked; Edition 2012 has not been confirmed