30CR13

11 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 30CR13 →

30Cr13 · GB /T 20878-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless and heat-resistant steels
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 20878—2007
Table / clause
Table 4, No. 102
PDF page references
13
Unit
Mass fraction (wt%)
Analysis type
Standard composition requirements

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Si≤ 1 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr12 ~ 14

Applicability and limitations

GB/T 20878—2007 tabulated chemical-composition mass fractions wt%; Values in parentheses are maximum permitted additions; conditional expressions require manual interpretation against the original text. Ni ≤0.60 is a maximum permitted addition shown in parentheses. A material-database match does not guarantee cold-heading suitability, actual supply or finished-product strength. GB/T 20878—2007 is a historical edition; This record does not replace verification of the current standard, contract or material applicability.

Verification notes

GB/T 20878—2007 historical original, Table 4, entry 102. The complete 45-page scan was checked. The standard is withdrawn; the historical edition’s application limits are retained.

30Cr13 · GB /T 1220-2007

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · GB /T 20878-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · GB /T 3280-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · GB /T 4237-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · GB /T 4240-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · GB /T 4356-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · GJB 2294A-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 0.8 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · JB /T 6908-2020

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · Q/RP 007-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

30Cr13 · Chinese national standard

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.26 ~ 0.35
Cr12 ~ 14
Mn≤ 1 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.