- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、5、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.7 (lower limit not stated) |
| Fe | ≤ 0.7 (lower limit not stated) |
| Cu | 3.8 ~ 4.8 |
| Mn | 0.4 ~ 0.8 |
| Mg | 0.4 ~ 0.8 |
| Ni | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.3 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass fraction %; unspecified elements are not treated as zero. This standard specifies the chemical composition of wrought aluminium and aluminium alloys; it does not automatically establish cold-heading suitability, actual supply, or finished-product performance. Al is the balance; the original table gives no independent numerical range for Al. Individual and total limits for other impurities apply only to the other elements referred to in clause 4.3, not to the sum of all principal alloying elements; a missing impurity test is not zero.
Combined limits
- Combined-element limits
- Requirement
- Fe+Ni (GB/T 3190—1996, Table 1)
- Element coefficient
- Fe
- 1
- Ni
- 1
- Lower limit
- Not stated
- Upper limit
- 0.7
- Elements requiring measured values from the same heat
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.1
- Other impurities require technical review
- Yes