← BackMaterial grade directory

2A02

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 2A02 →

2A02 · GB/T 3190—1996

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Aluminum and aluminum alloys
Subcategory
Aluminum and aluminum alloys
Material form
Reference record
Original record status
Original-standard record
Standard edition
GB/T 3190—1996
Table / clause
Table 1; Clause 4.1~4.5 · Footnotes
PDF page references
3、5、13

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Si≤ 0.3 (lower limit not stated)
Fe≤ 0.3 (lower limit not stated)
Cu2.6 ~ 3.2
Mn0.45 ~ 0.7
Mg2.0 ~ 2.4
Zn≤ 0.1 (lower limit not stated)
Ti≤ 0.15 (lower limit not stated)

Applicability and limitations

GB/T 3190—1996, Table 1, mass fraction %; unspecified elements are not treated as zero. This standard specifies the chemical composition of wrought aluminium and aluminium alloys; it does not automatically establish cold-heading suitability, actual supply, or finished-product performance. Al is the balance; the original table gives no independent numerical range for Al. Individual and total limits for other impurities apply only to the other elements referred to in clause 4.3, not to the sum of all principal alloying elements; a missing impurity test is not zero.

Combined limits

Other-impurity requirements in the source
Each other impurity
0.05
Sum of other impurities
0.1
Other impurities require technical review
Yes