27SIMN
4 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 27SIMN →27SiMn · GB/T 3077-1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 3077-1999
- Table / clause
- Table 1, item 8, note 2 and Table 2; 6.1.1.3
- PDF page references
- 3、4、7、8
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.32 |
| Si | 1.1 ~ 1.4 |
| Mn | 1.1 ~ 1.4 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
Original 1999 edition heat analysis wt%; Save quality/high-quality A/extra-high-quality E and Table 2 phosphorus and sulfur residual requirements separately according to Table 1 Note 2. ; Clause 6.1.1.3: For hot-pressure working, Cu≤.20%.; If hot working is not specified, this restriction is not applied by default. ; 6.1.1.2 Residual W/V/Ti shall be analyzed and recorded in the quality certificate; specific limits are per requirement, and unspecified values shall not be filled as zero. ; Product processing methods shall be specified in the contract; Cold-heading suitability cannot be proven solely by alloy structural steel composition; delivery condition/hot upsetting/surface shall be verified separately. ; Finished product tolerances in Clause 6.1.2 shall be verified separately per GB222 and shall not expand the default heat analysis range.
Verification notes
Original 1/2 table and quality-class notes were visually checked27SiMn · GB/T 3077-2015
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy structural steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 3077-2015
- Table / clause
- Tables 1 and 2; A/E designation rules in the endnote to Table 1
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.32 |
| Mn | 1.1 ~ 1.4 |
| Si | 1.1 ~ 1.4 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
Applicability and limitations
GB/T 3077-2015 Table 1 gives ladle analysis; Table 2 gives P/S and residual-element requirements. The final note to Table 1 allows ordering any grade as higher or special quality by adding A or E after the grade; this record is ordinary quality steel. For steel used in hot-pressure working, Cu ≤0.20%; the ordinary Cu maximum does not apply to this use. Explicit alloy ranges in Table 1 take priority; for Cr/Ni/Mo not specified there, use the residual limits in Table 2 and do not add residual limits on top of alloying-element ranges. Sn/Sb/As must be analyzed and recorded on the inspection certificate; any needed limits require agreement, and no generic numerical limits are invented here. Product-analysis deviations are handled separately under GB/T 222 and do not directly expand ladle limits. Mechanical properties depend on specimen dimensions and the recommended heat-treatment/delivery condition; this composition review does not constitute verification of properties.
Verification notes
Tables 1/2 and quality-grade rules checked27SiMn · GB/T 3078-2019
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy structural steel
- Material form
- Cold-drawn bars
- Original record status
- Original standard verified
- Standard edition
- GB/T 3078-2019
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.32 |
| Si | 1.1 ~ 1.4 |
| Mn | 1.1 ~ 1.4 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
Applicability and limitations
GB/T3078-2019, Clause 7.1.1: Quality carbon structural steel refers to GB/T699; alloy structural steel refers to GB/T3077.; The source of chemical composition must simultaneously display the referenced standard. ; Applies to cold-drawn steel bars and cold-drawn polished round bars.; Apply product-analysis tolerances under GB/T222 separately; do not incorporate them directly into heat-analysis ranges.. ; GB/T3077-2015 Table 2: This unsuffixed grade uses the quality-steel limits P/S≤0.030%, Cu≤0.30%, with Cu≤0.20% for hot working.; A/E quality grades are retained separately and shall not be merged under the same grade. ; Cr/Ni/Mo in Table 2 are residual element upper limits; For elements with specified alloy ranges in Table 1, use the Table 1 ranges; do not also apply conflicting residual upper limits.. ; Sn/Sb/As shall be analyzed and recorded in the quality certificate; limits shall be agreed upon when required, as the standard does not provide general values here.
Verification notes
The cited clauses in 3078 and the original texts of the referenced standards have been checked.Hardness in the delivery condition (conditions shown separately)
GB/T 3078-2019 · Table 2 hardness in delivery condition and Note a; 7.3/7.4 · PDF pages 6, 7 · HBW
Standard condition data, not actual measured results of supplied heats; Actual delivery condition, application, and contract must be confirmed.
- Clause 7.3.1: The specific delivery condition shall be stated in the contract; if it is not specified, delivery shall be in the cold-drawn condition.
- 7.4.1 Hardness for delivery in the normalized condition shall be agreed by both parties; the two general-use columns in Table 2 do not apply to the normalized condition.
- Values in parentheses are for reference and are not acceptance criteria.
- 7.4.2 Hot-pressure-working applications are subject to separate limits; do not automatically apply the general condition in Table 2.
- 7.4.2 For hot-pressure working, supplied in the cold-drawn condition: 50Mn2, 35CrMnSi, 42CrMo and 35CrMoV per Table 2; 38CrSi and 38CrMoAl ≤285 HBW; other grades ≤269 HBW. Confirm the actual use; the ordinary Table 2 condition cannot replace this condition.
- 7.4.3 No hardness test is performed when the nominal cross-sectional dimension (diameter, thickness or diagonal length) is below 5 mm. At the purchaser’s request, stated in the contract, tensile strength may be used instead of hardness; the specific requirements shall be agreed by both parties. This clause provides no automatic conversion relationship.
Cold-drawn or cold-drawn and bright-polished delivery; Table 2 conditions are for general use. For hot-pressure-working applications, check clause 7.4.2 separately.
HBW:≤ 255 (lower limit not stated) HBW
Delivery in the annealed, bright-annealed, high-temperature-tempered or tempered-after-normalizing condition; delivery as-normalized is excluded and shall be agreed by both parties under 7.4.1.
HBW:≤ 217 (lower limit not stated) HBW
27SiMn · GB /T 11251-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Alloy steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.32 |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | 1.1 ~ 1.4 |
| Mo | ≤ 0.1 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | 1.1 ~ 1.4 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.