27CRNIMOH
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 27CRNIMOH →27CrNiMoH · GB/T 5216-2014
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5216-2014
- Table / clause
- Table 1 and notes a/b; clauses 6.1.1–6.1.4
- PDF page references
- 1、7、9
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Typically, residual Cu ≤0.25%; default S ≤0.035%
Normally residual Cu ≤0.25%; at the purchaser’s request, S is 0.015–0.035% (the ±0.005% product-analysis tolerance for S must be checked separately).
For hot-pressure working, Cu≤0.20%; default S≤0.035%.
For hot-pressure working, Cu≤0.20%; S 0.015–0.035% only when required by the purchaser (product-analysis tolerance ±0.005 to be checked separately).
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.3 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.6 ~ 0.95 |
| Cr | 0.35 ~ 0.65 |
| Ni | 0.35 ~ 0.75 |
| Mo | 0.15 ~ 0.25 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| O | ≤ 0.002 (lower limit not stated) |
Applicability and limitations
Official GB/T5216-2014, cover PDF1, Clause 6.1 PDF7, Table 1 and footnotes PDF8/9; Heat-analysis mass fractions wt%. ; Clause 6.1.2 residual Cu≤.25, Cr≤.30, Ni≤.30%; Specified alloy ranges in the table shall take priority; Hot working Cu≤.20 separate condition. ; 6.1.3 O≤.0020%; Unspecified residual limits such as Mo must not be assumed zero. ; Note a: Only for 16CrMnH/20CrMnH/25CrH/28CrH, Si≤.12% may be agreed at the buyer's request; the effect on mechanical properties must be considered.. ; Note b: Per buyer's request, S may be .015–.035%; in this case, the finished product tolerance is ±.005%, which is not a default heat analysis relaxation. ; H/HH/HL are different hardenability bands; S denotes a sulfur-related grade-designation condition.; Only compositions of H grades are listed this time; hardenability curves and all mechanical properties are not claimed to have been verified. ; The intended use for metal forming or machining under this standard must be stated in the contract.; Cold heading, annealing and actual wire-rod supply require separate confirmation; do not automatically add products..
Original condition-branch records
Typically, residual Cu ≤0.25%; default S ≤0.035%
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.3 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.6 ~ 0.95 |
| Cr | 0.35 ~ 0.65 |
| Ni | 0.35 ~ 0.75 |
| Mo | 0.15 ~ 0.25 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| O | ≤ 0.002 (lower limit not stated) |
Normally residual Cu ≤0.25%; at the purchaser’s request, S is 0.015–0.035% (the ±0.005% product-analysis tolerance for S must be checked separately).
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.3 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.6 ~ 0.95 |
| Cr | 0.35 ~ 0.65 |
| Ni | 0.35 ~ 0.75 |
| Mo | 0.15 ~ 0.25 |
| P | ≤ 0.03 (lower limit not stated) |
| S | 0.015 ~ 0.035 |
| Cu | ≤ 0.25 (lower limit not stated) |
| O | ≤ 0.002 (lower limit not stated) |
For hot-pressure working, Cu≤0.20%; default S≤0.035%.
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.3 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.6 ~ 0.95 |
| Cr | 0.35 ~ 0.65 |
| Ni | 0.35 ~ 0.75 |
| Mo | 0.15 ~ 0.25 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| O | ≤ 0.002 (lower limit not stated) |
For hot-pressure working, Cu≤0.20%; S 0.015–0.035% only when required by the purchaser (product-analysis tolerance ±0.005 to be checked separately).
| Element | Composition requirement |
|---|---|
| C | 0.24 ~ 0.3 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.6 ~ 0.95 |
| Cr | 0.35 ~ 0.65 |
| Ni | 0.35 ~ 0.75 |
| Mo | 0.15 ~ 0.25 |
| P | ≤ 0.03 (lower limit not stated) |
| S | 0.015 ~ 0.035 |
| Cu | ≤ 0.2 (lower limit not stated) |
| O | ≤ 0.002 (lower limit not stated) |