Open condition selection, comparison and carbon-equivalent tools for 25CR2MO1VA →25Cr2Mo1VA · GB/T 3077-2015
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy structural steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 3077-2015
- Table / clause
- Tables 1 and 2; A/E designation rules in the endnote to Table 1
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.22 ~ 0.29 |
| Mn | 0.5 ~ 0.8 |
| Cr | 2.1 ~ 2.5 |
| Mo | 0.9 ~ 1.1 |
| Si | 0.17 ~ 0.37 |
| V | 0.3 ~ 0.5 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
Applicability and limitations
GB/T 3077-2015 Table 1 gives ladle analysis; Table 2 gives P/S and residual-element requirements. The final note to Table 1 allows ordering any grade as higher or special quality by adding A or E after the grade; this record is higher-quality steel. For steel used in hot-pressure working, Cu ≤0.20%; the ordinary Cu maximum does not apply to this use. Explicit alloy ranges in Table 1 take priority; for Cr/Ni/Mo not specified there, use the residual limits in Table 2 and do not add residual limits on top of alloying-element ranges. Sn/Sb/As must be analyzed and recorded on the inspection certificate; any needed limits require agreement, and no generic numerical limits are invented here. Product-analysis deviations are handled separately under GB/T 222 and do not directly expand ladle limits. Mechanical properties depend on specimen dimensions and the recommended heat-treatment/delivery condition; this composition review does not constitute verification of properties.
Verification notes
Tables 1/2 and quality-grade rules checked25Cr2Mo1VA · GB/T 3077-1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy structural steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 3077-1999
- Table / clause
- Table 1, No. 45 and notes 1–4; Table 2; 6.1.1–6.1.2
- PDF page references
- 5、7、8
- Unit
- Mass fraction (wt%)
- Analysis type
- Heat analysis, not product analysis
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
High-grade quality steel; For machining or processes other than hot pressure working, the maximum in Table 2Cu applies
High-grade quality steel; Hot pressure working, 6.1.1.3 Cu≤0.20%
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.22 ~ 0.29 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.5 ~ 0.8 |
| Cr | 2.1 ~ 2.5 |
| Mo | 0.9 ~ 1.1 |
| V | 0.3 ~ 0.5 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
Applicability and limitations
GB/T 3077—1999 Table 1 heat analysis mass fraction wt%; This record is based on the actual 1999 edition and shall not be replaced by the 2015 edition.. Grades marked A in the table are ordered as high-quality steel.; P/S/Cu and residual Mo in Table 2 are according to the corresponding quality grade.; Residual Cr/Ni/Mo limits do not cover alloy compositions already listed in Table 1.. The chemical compositions of this standard are also applicable to steel ingots, blooms, and their products.; Bar product ranges and mechanical properties/surface quality requirements cannot be directly extended as guarantees for wire cold-heading.. If the processing purpose is not specified in the contract, it shall be treated as machining.; Cu ≤ 0.20% during hot working; please select the corresponding condition.. Clause 6.1.1.2: Residual W/V/Ti shall be analyzed and recorded in the quality certificate; where no unified limit is listed, do not fill in 0.; Alloy W/V/Ti ranges in Table 1 are still retained.. Upgrading to A/E quality or specifying separate compositions according to Table 1 Note 2 requires separate order verification; grades shall not be automatically merged, nor shall the C range of this line be rewritten.. Rare earth 0.05% in Table 1 Note 4 is the calculated addition amount; finished product analysis is for reference only and shall not serve as a guaranteed composition range.. Analysis deviations for finished steel or bloom products shall be verified separately according to the referenced GB/T222–1984; heat analysis limits shall not be automatically relaxed..
Original condition-branch records
High-grade quality steel; For machining or processes other than hot pressure working, the maximum in Table 2Cu applies
| Element | Composition requirement |
|---|---|
| C | 0.22 ~ 0.29 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.5 ~ 0.8 |
| Cr | 2.1 ~ 2.5 |
| Mo | 0.9 ~ 1.1 |
| V | 0.3 ~ 0.5 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
High-grade quality steel; Hot pressure working, 6.1.1.3 Cu≤0.20%
| Element | Composition requirement |
|---|---|
| C | 0.22 ~ 0.29 |
| Si | 0.17 ~ 0.37 |
| Mn | 0.5 ~ 0.8 |
| Cr | 2.1 ~ 2.5 |
| Mo | 0.9 ~ 1.1 |
| V | 0.3 ~ 0.5 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |