2024
9 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 2024 →2024 · GB /T 3190-2008
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original text of the historical edition verified
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、7、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Mn | 0.3 ~ 0.9 |
| Mg | 1.2 ~ 1.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass percent; Unspecified elements are not treated as zero. ; This standard covers chemical composition of wrought aluminum and aluminum alloys; This does not establish cold-heading suitability, actual supply or finished-product properties. ; Al is the balance; The original table specifies no independent numerical range for Al. ; Individual and combined limits for other impurities concern only the other elements defined in Clause 4.3 of the standard, not the sum of all principal alloying elements; Missing impurity test results must not be treated as zero. ; Table 1, footnote 3: only by purchaser-supplier agreement, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
Combined limits
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.15
- Other impurities require technical review
- Yes
- Conditional requirements in the source
- Footnote
- 3
- Source conditions
- Only when agreed between purchaser and supplier, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
- Automatic evaluation implemented
- No
Verification notes
The original GB/T 3190—1996, Table 1 is used as an explicitly historical basis; The 2008/2020 edition cited in the original index has not been verified.2024 · GB /T 3190-2020
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original text of the historical edition verified
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、7、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Mn | 0.3 ~ 0.9 |
| Mg | 1.2 ~ 1.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass percent; Unspecified elements are not treated as zero. ; This standard covers chemical composition of wrought aluminum and aluminum alloys; This does not establish cold-heading suitability, actual supply or finished-product properties. ; Al is the balance; The original table specifies no independent numerical range for Al. ; Individual and combined limits for other impurities concern only the other elements defined in Clause 4.3 of the standard, not the sum of all principal alloying elements; Missing impurity test results must not be treated as zero. ; Table 1, footnote 3: only by purchaser-supplier agreement, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
Combined limits
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.15
- Other impurities require technical review
- Yes
- Conditional requirements in the source
- Footnote
- 3
- Source conditions
- Only when agreed between purchaser and supplier, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
- Automatic evaluation implemented
- No
Verification notes
The original GB/T 3190—1996, Table 1 is used as an explicitly historical basis; The 2008/2020 edition cited in the original index has not been verified.2024 · JIS H 4040-2006
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- JIS H 4040:2006
- Table / clause
- Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
- PDF page references
- 8
- Unit
- Mass fraction (%)
- Analysis type
- Chemical composition (refer to the source notes for the analysis type)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Mn | 0.3 ~ 0.9 |
| Mg | 1.2 ~ 1.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
Table 2, footnote 3/4: Zr+Ti<=0.20 applies only by purchaser-supplier agreement and is not a default restriction. ; Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable forms: extruded bars, cold-drawn bars and cold-drawn wire; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.
Verification notes
2006: Tables 1 and 2 in the original Japanese edition corrected page by page and cell by cell; alloy designation 2024; original PDF page 8, Table 22024 · JIS H 4040-2015
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- JIS H 4040:2015
- Table / clause
- Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
- PDF page references
- 15
- Unit
- Mass fraction (%)
- Analysis type
- Chemical composition (refer to the source notes for the analysis type)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Mn | 0.3 ~ 0.9 |
| Mg | 1.2 ~ 1.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
Table 2, footnote c/d: Zr+Ti<=0.20 applies only by purchaser-supplier agreement and is not a default restriction. ; Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable forms: extruded bars, cold-drawn bars and cold-drawn wire; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.
Verification notes
2015: Tables 1 and 2 in the original English edition corrected page by page and cell by cell; alloy designation 2024; original PDF page 15, Table 22024 · GB/T 3190—1996
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、7、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 0.5 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Mn | 0.3 ~ 0.9 |
| Mg | 1.2 ~ 1.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass percent; Unspecified elements are not treated as zero. ; This standard covers chemical composition of wrought aluminum and aluminum alloys; This does not establish cold-heading suitability, actual supply or finished-product properties. ; Al is the balance; The original table specifies no independent numerical range for Al. ; Individual and combined limits for other impurities concern only the other elements defined in Clause 4.3 of the standard, not the sum of all principal alloying elements; Missing impurity test results must not be treated as zero. ; Table 1, footnote 3: only by purchaser-supplier agreement, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
Combined limits
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.15
- Other impurities require technical review
- Yes
- Conditional requirements in the source
- Footnote
- 3
- Source conditions
- Only when agreed between purchaser and supplier, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
- Automatic evaluation implemented
- No
2024 · SAE AMS-QQ-A-250
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | ≤ 0.1 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Fe | ≤ 0.5 (lower limit not stated) |
| Mg | 1.2 ~ 1.8 |
| Mn | 0.3 ~ 0.9 |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
2024 · GB /T 3195-2016
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | ≤ 0.1 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Fe | ≤ 0.5 (lower limit not stated) |
| Mg | 1.2 ~ 1.8 |
| Mn | 0.3 ~ 0.9 |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
2024 · GB /T 3880.1-2012
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | ≤ 0.1 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Fe | ≤ 0.5 (lower limit not stated) |
| Mg | 1.2 ~ 1.8 |
| Mn | 0.3 ~ 0.9 |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
2024 · GJB 1741-1993
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | ≤ 0.1 (lower limit not stated) |
| Cu | 3.8 ~ 4.9 |
| Fe | ≤ 0.5 (lower limit not stated) |
| Mg | 1.2 ~ 1.8 |
| Mn | 0.3 ~ 0.9 |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.