2014
3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 2014 →2014 · GB/T 3190—1996
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Aluminum and aluminum alloys
- Subcategory
- Aluminum and aluminum alloys
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- GB/T 3190—1996
- Table / clause
- Table 1; Clause 4.1~4.5 · Footnotes
- PDF page references
- 3、7、13
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | 0.5 ~ 1.2 |
| Fe | ≤ 0.7 (lower limit not stated) |
| Cu | 3.9 ~ 5.0 |
| Mn | 0.4 ~ 1.2 |
| Mg | 0.2 ~ 0.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
GB/T 3190—1996, Table 1, mass percent; Unspecified elements are not treated as zero. ; This standard covers chemical composition of wrought aluminum and aluminum alloys; This does not establish cold-heading suitability, actual supply or finished-product properties. ; Al is the balance; The original table specifies no independent numerical range for Al. ; Individual and combined limits for other impurities concern only the other elements defined in Clause 4.3 of the standard, not the sum of all principal alloying elements; Missing impurity test results must not be treated as zero. ; Table 1, footnote 3: only by purchaser-supplier agreement, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
Combined limits
- Other-impurity requirements in the source
- Each other impurity
- 0.05
- Sum of other impurities
- 0.15
- Other impurities require technical review
- Yes
- Conditional requirements in the source
- Footnote
- 3
- Source conditions
- Only when agreed between purchaser and supplier, Ti+Zr content in extruded and forged products is limited to no more than 0.20%.
- Automatic evaluation implemented
- No
2014 · JIS H 4040-2015
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- JIS H 4040:2015
- Table / clause
- Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
- PDF page references
- 15
- Unit
- Mass fraction (%)
- Analysis type
- Chemical composition (refer to the source notes for the analysis type)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | 0.5 ~ 1.2 |
| Fe | ≤ 0.7 (lower limit not stated) |
| Cu | 3.9 ~ 5.0 |
| Mn | 0.4 ~ 1.2 |
| Mg | 0.2 ~ 0.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
Table 2, footnote b: Be≤0.0003% applies only to filler rods and welding wire; it is not a default restriction for all forms. ; Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable forms: extruded bars and cold-drawn bars; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.
Verification notes
2015: Tables 1 and 2 in the original English edition corrected page by page and cell by cell; alloy designation 2014; original PDF page 15, Table 22014 · JIS H 4040-2006
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- JIS H 4040:2006
- Table / clause
- Table 1: applicable product forms and designations; Table 2: chemical composition and footnotes.
- PDF page references
- 8
- Unit
- Mass fraction (%)
- Analysis type
- Chemical composition (refer to the source notes for the analysis type)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Si | 0.5 ~ 1.2 |
| Fe | ≤ 0.7 (lower limit not stated) |
| Cu | 3.9 ~ 5.0 |
| Mn | 0.4 ~ 1.2 |
| Mg | 0.2 ~ 0.8 |
| Cr | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.25 (lower limit not stated) |
| Ti | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
Table 2, footnote 2: Be≤0.0003% applies only to filler rods and welding wire; it is not a default restriction for all forms. ; Al is the balance; no independent numerical minimum is specified; Subtracting listed maxima from 100% must not be used to invent a minimum. ; Each otherwise unlisted element is ≤0.05%; this is not automatically treated as a known limit for a specific element. ; The combined total of otherwise unlisted elements is ≤0.15%. ; Table 1 applicable forms: extruded bars and cold-drawn bars; Form codes correspond only to Table 1 of this edition and do not establish supply by Creation Group. ; Table 2 gives chemical composition in mass percent; Mechanical properties, dimensions and delivery condition require separate verification against the applicable original tables and order requirements.