18CRNIMO7

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 18CRNIMO7 →

18CrNiMo7 · ISO 683-18-1996

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Case-hardening steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ISO 683-18-1996
Table / clause
Table3 and footnote 1–5; 7.2.2.1–7.2.2.2
PDF page references
6、11、12、13

Source document

Carbon-equivalent reference

IIW / CEV:0.6517–0.8617Known-element contribution; incomplete value; missing V, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2875–0.3975Known-element contribution; incomplete value; missing Cu, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3200–0.4425Known-element contribution; incomplete value; missing Cu CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.15 ~ 0.21
Si0.15 ~ 0.4
Mn0.35 ~ 0.65
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cr1.5 ~ 1.8
Mo0.25 ~ 0.35
Ni1.4 ~ 1.7

Applicability and limitations

ISO 683-18:1996 Bright non-alloy and low-alloy steel products, Table 3 Heat analysis of carburizing steels, mass fraction wt%; This is not a composition confirmation of the 2014 edition. ; This source is a 13-page public excerpt from the official version; complete composition rows and 5 footnotes from Table 3 have been obtained.; Without Table 4 product-analysis tolerances, Tables 7/8 hardenability data and Chapter 8 compositions of steels for quenching and tempering, verification of the entire standard must not be claimed complete.. ; Currently displaying the range for common grades in Table 3. When hardenability requirements are specified, Footnote 1 allows limited deviations except for P/S, with C not exceeding ±0.01% and other elements subject to Table 4; The absence of Table 4 shall not automatically relax ranges, nor shall it be used for the acceptance of H grades. ; Machinability may be improved by adding lead or controlling sulfide shape upon request; Where lead values are not specified, they shall not be filled as zero or assigned an arbitrary range. ; For other carburizing steels, see ISO 683-11:1987; Different suffix names in the 2014 edition shall not be automatically regarded as the same grade in the 1996 edition. ; A lower Si may be agreed upon during inquiry and ordering, provided the impact on mechanical properties is considered; The base ranges in Table 3 are currently used; do not remove the Si lower limit arbitrarily.. ; Elements not listed in the table must not be assumed to have zero content.; Unlisted elements shall not be intentionally added without the buyer's consent (except additions needed to finish steelmaking), and elements affecting properties introduced via scrap steel etc. shall be prevented. ; Clause 7.2.2.1 stipulates that Table 3 is used for heat analysis; Product-analysis tolerances are given in Table 4, which has not been obtained.. Clause 5.1.2 requires killed steel. Carbide spheroidizing annealing conditions required for cold-heading/cold-extrusion are covered separately by ISO 4954; cold-heading applicability cannot be determined solely by composition.

Verification notes

All rows, merged cells and footnotes in the publicly available official-edition excerpt, Table 3 were visually checked item by item; Only ordinary-grade heat composition has been confirmed
WhatsApp Technical enquiry →