← BackMaterial grade directory

17MNCR5

4 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 17MNCR5 →

17MnCr5 · ISO 683-17-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Bearing steel
Subcategory
Bearing steel
Material form
Reference record
Composition basis
Standard heat-analysis composition
Original record status
Original standard verified
Standard edition
ISO 683-17-2014
Table / clause
Table 3 and footnotes a–k
PDF page references
14、16
Unit
mass fraction (wt%)
Analysis type
Heat analysis; oxygen analysis is separately subject to the manufacturer’s choice

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default heat-analysis composition in the original table; Manufacturer option: oxygen in heat analysis ≤0.002%
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in heat analysis ≤0.002%
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat-analysis composition in the original table; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

ISO 683-17:2014 Table 3 and footnotes checked against the original; Table 3 specifies heat analysis, mass fraction wt%; unspecified elements are not treated as zero. Product-analysis deviations are addressed separately in Table 4 and do not expand the default heat-analysis limits.

Composition conditions

Conditional requirement

Original condition-branch records

Default heat-analysis composition in the original table; Manufacturer option: oxygen in heat analysis ≤0.002%

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Oxygen-analysis conditions
Heat analysis

Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in heat analysis ≤0.002%

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Oxygen-analysis conditions
Heat analysis

Default heat-analysis composition in the original table; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Oxygen-analysis conditions
Product analysis
Separate product oxygen-analysis requirement
Element
O
Upper limit
0.002
Unit
wt%
Analysis type
Product analysis

Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Oxygen-analysis conditions
Product analysis
Separate product oxygen-analysis requirement
Element
O
Upper limit
0.002
Unit
wt%
Analysis type
Product analysis

A condition branch must be selected

Yes

Verification notes

This batch was reconciled against the 2015 DIN German original images and 2014 ISO English original images; edition-specific sources were kept separate, and outdated grades, values and footnote scopes were corrected.

17MnCr5 · DIN EN ISO 683-17-2015

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Bearing steel
Subcategory
Bearing steel
Material form
Reference record
Composition basis
Standard heat-analysis composition
Original record status
Original standard verified
Standard edition
DIN EN ISO 683-17:2015-02
Table / clause
Table 3 and footnotes a–k
PDF page references
18、19
Unit
mass fraction (wt%)
Analysis type
Heat analysis; oxygen analysis is separately subject to the manufacturer’s choice

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default heat-analysis composition in the original table; Manufacturer option: oxygen in heat analysis ≤0.002%
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in heat analysis ≤0.002%
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat-analysis composition in the original table; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

DIN EN ISO 683-17:2015-02 Table 3 and footnotes checked against the original; the original Table 3 specifies heat analysis, mass fraction wt%; unspecified elements are not treated as zero. Product-analysis deviations are addressed separately in Table 4 and do not expand the default heat-analysis limits.

Composition conditions

Conditional requirement

Original condition-branch records

Default heat-analysis composition in the original table; Manufacturer option: oxygen in heat analysis ≤0.002%

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Oxygen-analysis conditions
Heat analysis

Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in heat analysis ≤0.002%

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
O≤ 0.002 (lower limit not stated)
Oxygen-analysis conditions
Heat analysis

Default heat-analysis composition in the original table; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Oxygen-analysis conditions
Product analysis
Separate product oxygen-analysis requirement
Element
O
Upper limit
0.002
Unit
wt%
Analysis type
Product analysis

Default heat-analysis composition in the original table; Machinability by agreement: S≤0.030%; Manufacturer option: oxygen in product analysis ≤0.002%; not for judging heat-analysis oxygen

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.4 (lower limit not stated)
Mn1.0 ~ 1.3
P≤ 0.025 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr0.8 ~ 1.1
Al≤ 0.05 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Oxygen-analysis conditions
Product analysis
Separate product oxygen-analysis requirement
Element
O
Upper limit
0.002
Unit
wt%
Analysis type
Product analysis

A condition branch must be selected

Yes

Verification notes

This batch was reconciled against the 2015 DIN German original images and 2014 ISO English original images; edition-specific sources were kept separate, and outdated grades, values and footnote scopes were corrected.

17MnCr5 · ASTM A534-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
Al≤ 0.05 (lower limit not stated)
C0.14 ~ 0.19
Cr0.8 ~ 1.1
Cu≤ 0.3 (lower limit not stated)
Mn1 ~ 1.3
O≤ 0.002 (lower limit not stated)
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.4 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

17MnCr5 · DIN 17230-1980

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C0.14 ~ 0.19
Cr0.8 ~ 1.1
Cu≤ 0.3 (lower limit not stated)
Mn1 ~ 1.3
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Si≤ 0.4 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →