17B2
6 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 17B2 →17B2 · EN 10263
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Drawn wire
- Original record status
- Reference transcription of standard
- Standard edition
- BS EN 10263-4:2017
- Table / clause
- Table 4
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
Applicability and limitations
Heat analysis; see the source page for footnotes and agreement-based options. An unspecified range is not zero. The early temporary 2001 extraction has been replaced with the 2017 original. The website does not state an edition; this entry shows the edition of its source and does not establish contractual applicability.
Verification notes
Standard source: BS EN 10263-4:2017 · Table 4View associated products →17B2 · ISO 4954
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Cold-heading wire
- Original record status
- Reference transcription of standard
- Standard edition
- ISO 4954:2018
- Table / clause
- Table C.3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
ISO 4954:2018; heat analysis, mass fraction %; values without a stated range are upper limits; see the source page for complete table footnotes. The website does not specify the edition; the source edition is shown here and does not establish contractual applicability.
Verification notes
Standard source: ISO 4954:2018 · Table C.3View associated products →17B2 · ISO 4954-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Steel for quenching and tempering
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ISO 4954:2018
- Table / clause
- Table C.3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
ISO 4954:2018, Table C.3 gives heat analysis; A single value is a maximum; a dash is not zero. ; Product-analysis tolerances are listed separately under Table 2/3 of the standard and do not directly widen the heat-analysis composition ranges. ; Optional Al0.020–0.050% to improve cold-heading performance; this is not a universal mandatory minimum. ; Low Si may be agreed in the order, taking hardenability into account; Where hardenability is required, the standard permits limited deviations, except for P/S; C must not exceed 0.01%; see Table 2 for the other requirements. ; When a Cr maximum of 0.30% is specified, a minimum Cr may be agreed at ordering; 30MoB1 requires guaranteed hardenability, with Cr minimum 0.15% and an upper limit adjustable by agreement.
Verification notes
The original standard, Table C.3 and footnotes have been checked17B2 · EN 10263-4-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10263-4-2017
- Table / clause
- Table 4 and notes
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Default heat composition listed in the table; optional Al addition not selected.
Note 3: optional Al addition of 0.020–0.050% to improve cold-heading performance.
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
Applicability and limitations
EN10263-4:2017, Table 4, heat analysis, mass percent. ; Elements not listed shall not be filled as 0; they shall not be intentionally added without the consent of the purchaser, except additions needed to finish steelmaking. ; Note 2 allows the specification of small deviations when hardenability requirements exist, but this does not involve P/S; The default composition range is not expanded here; it must be combined with specific hardenability ordering conditions. ; Note 3 allows Al 0.020–0.050% to be listed separately; it shall not be defaulted as mandatory aluminum content. ; Mechanical properties and delivery conditions are to be verified separately; the standard range is not a guarantee for the forming of arbitrary parts. ; The text of Table 4 Note a indicates that a Cr lower limit may be agreed upon for grades with Cr≤.30%; the table header Footnote a is located at Si; the ambiguity of the original position is retained, and clear Si table values shall not be changed nor low Si conditions arbitrarily set based on this. ; The Cr lower limit of .15 in Table 4 Note b applies only to the core hardenability requirements of 1.5408 (30MoB1) and shall not be applied to other grades such as 30MnB4; Agreement to reduce the Cr upper limit must include a specific limit value.
Original condition-branch records
Default heat composition listed in the table; optional Al addition not selected.
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
Note 3: optional Al addition of 0.020–0.050% to improve cold-heading performance.
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
| Al | 0.02 ~ 0.05 |
A condition branch must be selected
YesVerification notes
Visual check of Tables 3 and 4 and footnotes in the English original17B2 · DIN EN 10263-4-2002
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10263-4-2002
- Table / clause
- Table 3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
Applicability and limitations
DIN EN10263-4:2002-02 adopts EN10263-4:2001; the edition relationship is expressly identified on the cover; Heat-analysis mass percentages. ; Historical Table 2/3 contains no optional Al addition note for 2017; newer-edition conditions are not applied. ; Table 2, note c permits an agreed carbon range of width .04%; tabulated defaults are unchanged without a specific agreement. ; Table 2, note d and Table 3, note c permit agreed lower Si, considering effects on properties/hardenability; no range is invented where none is specified. ; Unlisted elements are not entered as zero; Table 2, note a: intentional additions without purchaser consent are prohibited except to finish the heat; residuals may be present but must not impair properties. ; Table 2, note b permits specified deviations where hardenability is required, except for P/S; The default composition range is not widened here. ; Mechanical properties, delivery and hardenability require separate verification; suitability for forming a specific component requires separate confirmation. ; Historical Table 3, note d: minima for grades with Cr≤.30 may be agreed, but no general value is given; the 30MoB1 core-hardening .15 option from 2017 is not copied.
Verification notes
Older-edition Tables 2 and 3 and footnotes visually checked; equivalence to the newer edition is not assumed.17B2 · Q/ZNGF 01.7—2023
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- 2023 Edition; Published 2023-09-21, implemented 2023-10-01; Supersedes Q/SG18—2022
- Document title
- Steel wire rod for cold heading and cold extrusion
- Table / clause
- Table 1
- PDF page references
- 6
- Unit
- Mass fraction (wt%)
- Manufacturer
- Guangdong Zhongnan Iron & Steel Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.2 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| B | 0.0008 ~ 0.005 |
| Cr | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Zhongnan Steel Q/ZNGF 01.7—2023, Table 1, row 63 (PDF page 6), cast analysis wt%; footnotes, delivery process and orders must be confirmed against the corresponding edition. This does not constitute a supply commitment by Creation Group.
Composition conditions
- Table 1 heat analysis, mass fractions wt%; A dash means no limit is listed, not zero.
- Clause 6.1.4 residual impurities Cr, Ni and Cu are each ≤0.20%; Where Cr is intentionally added, the corresponding row limits apply instead of residual maxima.