← BackMaterial grade directory

16CRMNAH

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 16CRMNAH →

16CrMnAH · GB/T 5216-2004

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5216-2004
Table / clause
Tables 1 and 2, notes a–c and clause 6.1; 15CrMoH includes Amendment No. 1
PDF page references
1、6、7

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Tables 1/2: default heat analysis
IIW / CEV:0.4667–0.6633Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3398Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3950Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account
IIW / CEV:0.4667–0.6633Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3315Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3950Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H
IIW / CEV:0.4667–0.6633Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3398Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3950Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H; Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account
IIW / CEV:0.4667–0.6633Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3315Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3950Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Hot pressure working Cu≤.20%
IIW / CEV:0.4667–0.6600Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3373Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3925Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Hot pressure working Cu≤.20%; Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account
IIW / CEV:0.4667–0.6600Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3290Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3925Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
For hot-pressure working, Cu≤0.20%; if the purchaser requires semi-free-cutting S at 0.020–0.035%, prefix the designation H with S.
IIW / CEV:0.4667–0.6600Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3373Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3925Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Hot pressure working Cu≤.20%; Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H; Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account
IIW / CEV:0.4667–0.6600Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2300–0.3290Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3925Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.37 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Applicability and limitations

GB/T 5216—2004 original Tables 1/2 and 6.1, ladle-analysis mass fraction wt%; retain the actual 2004 edition.

For high-quality steel, Note a to Table 1 adds A before H (e.g. 40CrAH); P/S by quality level and residual Cu/Cr/Ni follow Table 2; do not mix with the 2014 edition.

Under 6.1.3, Cu≤0.20% for hot-pressure processing. If the purchaser requires S 0.020–0.035%, add S before H; the sulfur tolerance ±0.005 is separately stated and does not expand the default range.

Table 1 alloy-element ranges take precedence over Table 2 residual limits; a blank means unspecified, not zero.

H/HH/HL hardenability bands, delivery condition, hardness and suitability for cold-heading processes require separate verification; this does not automatically create a supply product.

Original condition-branch records

Tables 1/2: default heat analysis

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.37 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.12 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.37 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.25 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H; Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.12 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.25 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Hot pressure working Cu≤.20%

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.37 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Hot pressure working Cu≤.20%; Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.12 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

For hot-pressure working, Cu≤0.20%; if the purchaser requires semi-free-cutting S at 0.020–0.035%, prefix the designation H with S.

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.37 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Hot pressure working Cu≤.20%; Purchaser-specified semi-free-cutting S .020–.035%; prefix S is added before designation H; Si≤.12% is required by the purchaser, taking its effect on mechanical properties into account

ElementComposition requirement
C0.14 ~ 0.19
Si≤ 0.12 (lower limit not stated)
Mn1.0 ~ 1.3
Cr0.8 ~ 1.1
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.035
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

2004 original: all 24 rows, Table 2 and Amendment No. 1 visually checked; high-quality grade applied according to note a.