- Material category
- Stainless steel
- Subcategory
- Martensitic stainless and heat-resistant steels
- Material form
- Reference record
- Verification status
- Original printed discrepancy awaiting resolution
- Standard edition
- GB/T 20878—2007
- Table / clause
- Table 4, No. 129
- PDF page references
- 16
- Unit
- Mass fraction (wt%)
- Analysis type
- Standard composition requirements
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.16 |
| Si | ≤ 0.6 (lower limit not stated) |
| Mn | ≤ 0.6 (lower limit not stated) |
| P | Original prints 0.300%; pending textual verification |
| S | ≤ 0.03 (lower limit not stated) |
| Ni | 2.8 ~ 3.4 |
| Cr | 13 ~ 15 |
| W | 1.6 ~ 2.2 |
| Ti | ≤ 0.05 (lower limit not stated) |
| B | ≤ 0.004 (lower limit not stated) |
| V | 0.18 ~ 0.28 |
Applicability and limitations
GB/T 20878—2007 historical version; The P column in the original text is printed as 0.300%; the numerical dispute remains unresolved. This row does not participate in automatic composition reverse-checks and cannot be used as a material selection limit. Other listed elements are transcribed from the original version.
Composition conditions
- Original GB/T 20878—2007 composition, mass fractions wt%; Values in parentheses are maximum permitted additions.
- In this row of scanned original Table 4, P is clearly printed as 0.300%, conflicting with the 0.030% commonly seen in comparable records. The printed value is retained and marked for checking against a second original; it must not be used as a final material-selection limit.
- This standard does not guarantee cold-heading suitability or actual supply.
Verification notes
Original GB/T 20878—2007, Table 4, item 129 prints 0.300% in the P column, conflicting with other transcriptions; The value is not used as a material-selection or composition reverse-matching limit, pending an official correction or verification against a second original.Source uncertainties and differences
- Element
- P
- Source 1
- Item 129 in Table 4 of the original 2007 scan is printed 0.300%
- Source 2
- Other transcriptions commonly give 0.030%; no official erratum or second original suitable for cross-checking has yet been obtained
- Review conclusion
- Retain the original printing and prohibit automatic composition reverse-lookup matching; Enable only after manual verification