13Cr13Mo · GB /T 1221-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 1221-2007
Table / clause
Table 6 · Notes 1/2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.08 ~ 0.18
Si≤ 0.6 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr11.5 ~ 14
Mo0.3 ~ 0.6

Applicability and limitations

Heat analysis, mass fractions wt%; Permissible deviations for product chemical composition shall be separately verified according to GB/T222. ; All values in the table are maximum values except for ranges or minimum values; Values in brackets are the maximum values that may be added or allowed to be contained, and are not required to be added. ; Standard for heat-resistant steel bars; a grade name alone does not establish suitability for cold heading or availability as wire; Processing methods and delivery conditions must be specified in the contract. ; In Table 6, the brackets (0.60) for Ni represent the upper limit that may be added or allowed to be contained.

Verification notes

The original GB/T1221-2007 table and notes have been checked

13Cr13Mo · GB /T 20878-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless and heat-resistant steels
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 20878—2007
Table / clause
Table 4, No. 115
PDF page references
14
Unit
Mass fraction (wt%)
Analysis type
Standard composition requirements

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.08 ~ 0.18
Si≤ 0.6 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr11.5 ~ 14
Mo0.3 ~ 0.6
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

GB/T 20878—2007 tabulated chemical-composition mass fractions wt%; Values in parentheses are maximum permitted additions; conditional expressions require manual interpretation against the original text. Ni ≤0.60 and Cu ≤0.30 are maximum permitted additions shown in parentheses. A material-database match does not guarantee cold-heading suitability, actual supply or finished-product strength. GB/T 20878—2007 is a historical edition; This record does not replace verification of the current standard, contract or material applicability.

Verification notes

GB/T 20878—2007 historical original, Table 4, entry 115. The complete 45-page scan was checked. The standard is withdrawn; the historical edition’s application limits are retained.

13Cr13Mo · GB /T 1220-2007

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.08 ~ 0.18
Cr11.5 ~ 14
Mn≤ 1 (lower limit not stated)
Mo0.3 ~ 0.6
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.6 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

13Cr13Mo · GB /T 20878-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.08 ~ 0.18
Cr11.5 ~ 14
Cu≤ 0.3 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
Mo0.3 ~ 0.6
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.6 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

13Cr13Mo · GB /T 4356-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.08 ~ 0.18
Cr11.5 ~ 14
Mn≤ 1 (lower limit not stated)
Mo0.3 ~ 0.6
Ni≤ 0.6 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.6 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.