1370 · GB/T 3190—1996

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Aluminum and aluminum alloys
Subcategory
Aluminum and aluminum alloys
Material form
Reference record
Original record status
Original-standard record
Standard edition
GB/T 3190—1996
Table / clause
Table 1; Clause 4.1~4.5 · Footnotes
PDF page references
3、4、13

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Si≤ 0.1 (lower limit not stated)
Fe≤ 0.25 (lower limit not stated)
Cu≤ 0.02 (lower limit not stated)
Mn≤ 0.01 (lower limit not stated)
Mg≤ 0.02 (lower limit not stated)
Cr≤ 0.01 (lower limit not stated)
Zn≤ 0.04 (lower limit not stated)
Al≥ 99.7 (upper limit not stated)
Ca≤ 0.03 (lower limit not stated)
B≤ 0.02 (lower limit not stated)

Applicability and limitations

GB/T 3190—1996, Table 1, mass percent; Unspecified elements are not treated as zero. ; This standard covers chemical composition of wrought aluminum and aluminum alloys; This does not establish cold-heading suitability, actual supply or finished-product properties. ; Al is listed as a minimum content; Aluminum content is calculated by difference under Clause 4.1/4.2, using the specified inclusion thresholds and precision; unmeasured elements must not be treated as zero. ; Individual and combined limits for other impurities concern only the other elements defined in Clause 4.3 of the standard, not the sum of all principal alloying elements; Missing impurity test results must not be treated as zero.

Combined limits

Combined-element limits
  • Requirement
    V+Ti (GB/T 3190—1996, Table 1)
    Element coefficient
    V
    1
    Ti
    1
    Lower limit
    Not stated
    Upper limit
    0.02
Elements requiring measured values from the same heat
  • Ti
  • V
Purity calculation rules in the source
PDF page references
3
Purity from 99.00% to below 99.90%
Al = 100 minus the sum of all other elements present at ≥0.010%; before summing, express each element to 0.0X%.
Purity from 99.90% to 99.99%
Al = 100 minus the sum of all other elements present at ≥0.001%; before summing, express each element to 0.00X%, then round the result to 0.0X%.
Rounding rules
Follow GB/T 8170; do not treat unspecified elements as zero or apply ordinary remainder calculations directly.
Purity requires technical review
Yes
Other-impurity requirements in the source
Each other impurity
0.02
Sum of other impurities
0.1
Other impurities require technical review
Yes