- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- SAE J1268-2010
- Table / clause
- Table 2 · Notes 1–6; Clause 3/4
- PDF page references
- 1、2、4、5、6
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Open-hearth or basic-oxygen steel: P≤0.030/S≤0.040
Basic electric-furnace steel: P and S each ≤0.025%
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.42 ~ 0.49 |
| Mn | 1.45 ~ 2.05 |
| Si | 0.15 ~ 0.35 |
| Cu | ≤ 0.35 (lower limit not stated) |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.06 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.04 (lower limit not stated) |
Applicability and limitations
SAE J1268 MAY2010 official original Table 2 and notes 1–6, ladle analysis (wt%). Note 1 applies within the stated scope: cross-sectional area ≤0.13 m², width 460 mm and piece mass 4.5 t; product deviations are handled separately under J409 and are not added to default limits. Note 2 residual maxima Cu≤0.35/Ni≤0.25/Cr≤0.20/Mo≤0.06 apply only when the element is not specified; listed alloy ranges take priority. Note 3: open-hearth/oxygen steel P≤0.030/S≤0.040; basic electric-furnace steel P and S each ≤0.025. The original note 5 identifies E4340H/E9310H as electric-furnace steel. Note 6: boron steel B 0.0005–0.003%; do not add boron to ordinary grades without B. Retain the explicit H-grade to UNS mappings from the source; do not merge them with grades without H. Hardenability bands, grain size, cold-heading process and supply require separate verification.
Original condition-branch records
Open-hearth or basic-oxygen steel: P≤0.030/S≤0.040
| Element | Composition requirement |
|---|---|
| C | 0.42 ~ 0.49 |
| Mn | 1.45 ~ 2.05 |
| Si | 0.15 ~ 0.35 |
| Cu | ≤ 0.35 (lower limit not stated) |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.06 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.04 (lower limit not stated) |
Basic electric-furnace steel: P and S each ≤0.025%
| Element | Composition requirement |
|---|---|
| C | 0.42 ~ 0.49 |
| Mn | 1.45 ~ 2.05 |
| Si | 0.15 ~ 0.35 |
| Cu | ≤ 0.35 (lower limit not stated) |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.06 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
A condition branch must be selected
YesVerification notes
Official original Table 2: all 73 rows and footnotes visually checked.1345H · ASTM A304-2020
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Structural steel with guaranteed hardenability
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ASTM A304-2020
- Table / clause
- Table 1 · Footnotes; 1.1–1.2, 7.1
- PDF page references
- 1、2、3、5
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.42 ~ 0.49 |
| Mn | 1.45 ~ 2.05 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.04 (lower limit not stated) |
| Si | 0.15 ~ 0.35 |
| Cu | ≤ 0.35 (lower limit not stated) |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.06 (lower limit not stated) |
Applicability and limitations
ASTM A304—2020 Tables 1 and 2 and 7.1 specify ladle analysis, mass fraction (wt%); this is an excerpt from the published edition, not verification of the complete standard. The scope is hot-worked carbon, alloy and carbon-boron steel bars with hardenability requirements; the H suffix must not be omitted or treated automatically as an ordinary grade. Product-analysis tolerances in Table 1 note 3 must be checked separately against A29/A29M; tolerances and hardenability bands were not reproduced here, and composition alone does not establish compliance with all H-steel requirements. Unlisted elements are not zero; residual-element maxima not specified in Table 1 note 2 are included for the applicable elements. Table 1 note 2 is not automatically applied to Table 2. A leaded variant requires the separate L designation in the source; Pb 0.15–0.35% has not been added to ordinary H grades. The boron-steel footnote states an expected minimum boron content of 0.0005%; it is listed separately and is not presented as a composition acceptance limit. Chemistry outside this table requires agreement between purchaser and supplier. Inclusion in the standard-material database does not establish cold-heading supply capability or direct substitutability; processing and supply conditions must be confirmed separately.
Verification notes
PDF pages 1/2/3/5 visually checked; composition-table rows and footnotes extracted and verified separately.1345H · CHINA STEEL CORPORATION · Bars and Wire Rods Product Catalogue 2014-C1 / 7.1.19 SAE · Alloy steels · H (Edition unspecified)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy steel
- Material form
- Bars and wire rod
- Original record status
- Manufacturer source verified
- Document edition
- CAT.NO.3-BD-01-2014-C1 (stated on the back cover)
- Document title
- Bars and Wire Rods Product Catalogue
- Table / clause
- 7.1.19 SAE · Alloy steels · H (Edition unspecified)
- PDF page references
- 25
- Unit
- Mass fraction (%)
- Analysis type
- The original catalogue does not explicitly identify the analysis type for this table
- Manufacturer
- CHINA STEEL CORPORATION
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.42 ~ 0.49 |
| Mn | 1.45 ~ 2.05 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.04 (lower limit not stated) |
| Si | 0.15 ~ 0.35 |
| Cu | ≤ 0.35 (lower limit not stated) |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.06 (lower limit not stated) |
Applicability and limitations
China Steel bar and wire-rod catalogue CAT.NO.3-BD-01-2014-C1, PDF page 25
printed page 23, 7.1.19 SAE alloy H steel (edition not stated). The original catalogue does not explicitly identify the analysis type for this table. Historical manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition: residual Cu/Ni/Cr/Mo maxima are added only for elements unspecified in the main table and do not override principal alloy-composition ranges.
Composition conditions
- Historical manufacturer 2014-C1 catalogue, bars/wire rod; Where the referenced standard edition is not identified, a year is not borrowed from another catalogue; a catalogue is not upgraded to the official standard text.
- A dash or blank must not be treated as zero. Composition data do not establish completeness or applicability of a formula; mechanical properties and supply require separate verification.
- Residual Cu/Ni/Cr/Mo limits supplement only elements not specified in the main table; they do not override the principal alloy-element ranges.