← BackMaterial grade directory

12NI14

6 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 12NI14 →

12Ni14 · EN 10028-4-2017

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified
Classification basis (does not replace original-source composition verification)

Classified as alloy steel according to the listed steel standard system and existing sources; The EN10028-4 and ISO9328-4 specified in the same-name record for 12Ni14 belong to the nickel alloy steel system. The original-source verification status for this record’s chemical composition is retained.

Flat products of steel for pressure purposes - Part 4: Nickel alloy steels with specified low-temperature properties

EN10028-4:2017 Nickel alloy steels with specified low temperature properties

ISO9328-4:2018 Nickel-alloy steels with specified low temperature properties

GB/T18984-2016 Seamless steel pipes for low temperature service piping

DIN17210:1986 Case hardening steels

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Mn0.3 ~ 0.8
Ni3.25 ~ 3.75
P≤ 0.02 (lower limit not stated)
S≤ 0.005 (lower limit not stated)
Si≤ 0.35 (lower limit not stated)
V≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

12Ni14 · EN 10216-4-2013

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified
Classification basis (does not replace original-source composition verification)

Classified as alloy steel according to the listed steel standard system and existing sources; The EN10028-4 and ISO9328-4 specified in the same-name record for 12Ni14 belong to the nickel alloy steel system. The original-source verification status for this record’s chemical composition is retained.

Flat products of steel for pressure purposes - Part 4: Nickel alloy steels with specified low-temperature properties

EN10028-4:2017 Nickel alloy steels with specified low temperature properties

ISO9328-4:2018 Nickel-alloy steels with specified low temperature properties

GB/T18984-2016 Seamless steel pipes for low temperature service piping

DIN17210:1986 Case hardening steels

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Mn0.3 ~ 0.8
Ni3.25 ~ 3.75
P≤ 0.025 (lower limit not stated)
S≤ 0.005 (lower limit not stated)
Si0.15 ~ 0.35
V≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

12Ni14 · NF EN 10253-2-2007

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified
Classification basis (does not replace original-source composition verification)

Classified as alloy steel according to the listed steel standard system and existing sources; The EN10028-4 and ISO9328-4 specified in the same-name record for 12Ni14 belong to the nickel alloy steel system. The original-source verification status for this record’s chemical composition is retained.

Flat products of steel for pressure purposes - Part 4: Nickel alloy steels with specified low-temperature properties

EN10028-4:2017 Nickel alloy steels with specified low temperature properties

ISO9328-4:2018 Nickel-alloy steels with specified low temperature properties

GB/T18984-2016 Seamless steel pipes for low temperature service piping

DIN17210:1986 Case hardening steels

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Mn0.3 ~ 0.8
Ni3.25 ~ 3.75
P≤ 0.025 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si0.15 ~ 0.35
V≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

12Ni14 · ISO 9328-4-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified
Classification basis (does not replace original-source composition verification)

Classified as alloy steel according to the listed steel standard system and existing sources; The EN10028-4 and ISO9328-4 specified in the same-name record for 12Ni14 belong to the nickel alloy steel system. The original-source verification status for this record’s chemical composition is retained.

Flat products of steel for pressure purposes - Part 4: Nickel alloy steels with specified low-temperature properties

EN10028-4:2017 Nickel alloy steels with specified low temperature properties

ISO9328-4:2018 Nickel-alloy steels with specified low temperature properties

GB/T18984-2016 Seamless steel pipes for low temperature service piping

DIN17210:1986 Case hardening steels

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Mn0.3 ~ 0.8
Ni3.25 ~ 3.75
P≤ 0.02 (lower limit not stated)
S≤ 0.005 (lower limit not stated)
Si≤ 0.35 (lower limit not stated)
V≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

12Ni14 · ISO 9330-3-1997

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified
Classification basis (does not replace original-source composition verification)

Classified as alloy steel according to the listed steel standard system and existing sources; The EN10028-4 and ISO9328-4 specified in the same-name record for 12Ni14 belong to the nickel alloy steel system. The original-source verification status for this record’s chemical composition is retained.

Flat products of steel for pressure purposes - Part 4: Nickel alloy steels with specified low-temperature properties

EN10028-4:2017 Nickel alloy steels with specified low temperature properties

ISO9328-4:2018 Nickel-alloy steels with specified low temperature properties

GB/T18984-2016 Seamless steel pipes for low temperature service piping

DIN17210:1986 Case hardening steels

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Mn0.3 ~ 0.85
Ni3.25 ~ 3.75
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si0.15 ~ 0.35
V≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

12Ni14 · ISO 9330-5-2000

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified
Classification basis (does not replace original-source composition verification)

Classified as alloy steel according to the listed steel standard system and existing sources; The EN10028-4 and ISO9328-4 specified in the same-name record for 12Ni14 belong to the nickel alloy steel system. The original-source verification status for this record’s chemical composition is retained.

Flat products of steel for pressure purposes - Part 4: Nickel alloy steels with specified low-temperature properties

EN10028-4:2017 Nickel alloy steels with specified low temperature properties

ISO9328-4:2018 Nickel-alloy steels with specified low temperature properties

GB/T18984-2016 Seamless steel pipes for low temperature service piping

DIN17210:1986 Case hardening steels

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
Al≥ 0.02 (upper limit not stated)
C≤ 0.15 (lower limit not stated)
Mn0.3 ~ 0.8
Ni3.25 ~ 3.75
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.35 (lower limit not stated)
V≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →