← BackMaterial grade directory

12L15

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 12L15 →

12L15 · ASTM A29/A29M-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A29/A29M-2012
Table / clause
Table 1, footnotes A–G
PDF page references
1、3、4

Carbon-equivalent reference

IIW / CEV:0.1250–0.2650 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0375–0.1425Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0750–0.1950 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.09 (lower limit not stated)
Mn0.75 ~ 1.05
P0.04 ~ 0.09
S0.26 ~ 0.35
Pb0.15 ~ 0.35

Applicability and limitations

2012 original text Table 1 heat analysis mass fraction wt%; The applicability and deviations of product analysis must be separately confirmed according to 4.3 and Table 5. Grades and product forms are retained as listed in this standard; suitability for cold heading is not automatically guaranteed. Note D only specifies Pb 0.15–0.35% for lead-bearing 'L' grades; Standard grades without 'L' shall not automatically include Pb. Note F: Additions of Bi/Ca/Se/Te are subject to agreement between the supplier and purchaser; do not enter zero when no value is specified..

Verification notes

The 2012 Table 1 and footnotes have been checked; order-specific optional compositions and base-table limits remain separate.

12L15 · ASTM A29/A29M-2023

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A29/A29M-2023
Table / clause
Table 1, footnotes A–G
PDF page references
5
Unit
Mass fraction (wt%)
Analysis type
Heat analysis; When lead is added to the ladle stream, its cast/heat analysis cannot be determined

Carbon-equivalent reference

IIW / CEV:0.1250–0.2650 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0375–0.1425Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0750–0.1950 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.09 (lower limit not stated)
Mn0.75 ~ 1.05
P0.04 ~ 0.09
S0.26 ~ 0.35
Pb0.15 ~ 0.35

Applicability and limitations

Original ASTM A29/A29M-2023, Table 1: the basic table gives heat-analysis mass fractions wt%; Product-analysis tolerances require separate confirmation under 4.3 and Table 5 and are not added to heat-analysis limits. When 4.1.1 is ordered by a grade in this table, the corresponding heat-analysis limits must be met; Other ordered compositions require separate agreement under 4.1.2 and Table 3/4 and are not merged into this table. General requirements for hot-worked bars; chemistry alone does not establish cold-heading suitability, supply or mechanical properties. Note D: Pb for leaded steel is 0.15–0.35%; L must remain part of the grade identity and is not included in ordinary grades; If lead is added in the ladle stream, its cast or heat-analysis content cannot be determined. Note F: Bi/Ca/Se/Te is specified by purchaser-supplier agreement; Unspecified numerical values are not entered as zero. The 4.3.2 product-analysis tolerance restrictions for P and S do not apply to resulfurized or rephosphorized/resulfurized steels; Product-analysis tolerances are not added to heat-analysis limits. This record is excluded from automatic composition reverse matching because the lead-analysis condition remains unresolved.

Verification notes

Existing OCR of the four-page, 190-row original 2023 table was parsed cell by cell. All values were screened for differences against independent 2012 data and checked against the original 2023 images and footnotes; no values were filled from the older edition.